ASTM B601 Temper Codes for Copper Metal and Copper Alloys

Copper Temper Name ASTM Code
1/8 Hard H00
1/4 Hard H01
1/2 Hard H02
3/4 Hard H03
Hard H04
Extra Hard H06
Spring H08
Extra Spring H10
Special Spring H12
Ultra Spring H13
Super Spring H14
Extruded and Drawn H50
Pierced and Drawn H52
Light Drawn, Light Cold Rolled H55
Drawn General Purpose H58
Cold Heading and Forming H60
Rivet H63
Screw H64
Bolt H66
Bending H70
Hard Drawn H80
Medium Hard Drawn Electrical Wire H85
Hard Drawn Electrical Wire H86
As Finned H90
As Manufactured Tempers ASTM Code
As Sand Cast M01
As Centrifugal Cast M02
As Plaster Cast M03
As Pressure Die Cast M04
As Permanent Mold Cast M05
As Investment Cast M06
As Continuous Cast M07
As Hot Forged and Air Cooled M10
As Forged and Quenched M11
As Hot Rolled M20
As Hot Extruded M30
As Hot Pierced M40
As Hot Pierced and Rerolled M45

Cold Worked and Stress Relieved Tempers ASTM Code
H01 Temper and Stress Relieved HR01
H02 Temper and Stress Relieved HR02
H04 Temper and Stress Relieved HR04
H08 Temper and Stress Relieved HR08
H10 Temper and Stress Relieved HR10
As Finned HR20
Drawn and Stress Relieved HR50

Cold Rolled and order Strengthened Tempers ASTM Code
H04 Temper and Order Heat Treated HT04
H08 Temper and Order Heat Treated HT08

References

For more general information about over 2000 specific copper, brass, and bronze alloy data sheets in MatWeb, choose one of the following links, or use one of our search techniques to reach specific products:

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。