MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

COMSOL CD

SABIC Innovative Plastics LEXAN 915R Polycarbonate (North America)

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)
 Export data to your CAD/FEA program

Subcategory: Polycarbonate; Polymer; Thermoplastic

Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.

Material Notes:
Information provided by GE Plastics for their North American product line. MatWeb has a separate entry for the European data sheet.

No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.

Physical PropertiesMetricEnglishComments
Density1.2 g/cc0.0434 lb/in³ ASTM D 792
Linear Mold Shrinkage0.0075 - 0.0095 cm/cm0.0075 - 0.0095 in/in Flow, 0.125 inch; ASTM D 955
Melt Flow18 g/10 min18 g/10 min 300C/1.2 kgf (O); ASTM D 1238

Mechanical Properties
Tensile Strength @ Break62.1 MPa9000 psi Type I, 2.0 in/min; ASTM D 638
Tensile Strength @ Yield63.4 MPa9200 psi Type I, 2.0 in/min; ASTM D 638
Elongation at Break130 %130 % Type I, 2.0 in/min; ASTM D 638
Elongation at Yield6 %6 % Type I, 2.0 in/min; ASTM D 638
Tensile Modulus2.41 GPa349 ksi 2.0 in/min; ASTM D 638
Flexural Modulus2.46 GPa357 ksi 0.05 in/min, 2" span; ASTM D 790
Flexural Yield Strength93.8 MPa13600 psi 0.05 in/min, 2" span; ASTM D 790
Gardner Impact @ 23°C67.8 J50 ft-lb Instrumented Impact Total Energy, 73°F; ASTM D 3763
Izod Impact, Notched7.47 J/cm14 ft-lb/in 73F; ASTM D 256

Electrical Properties
Arc ResistanceMax 60 secMax 60 sec Tungsten (+/- 0.125 inch); PLC Code 7; ASTM D 495
Comparative Tracking IndexMin 600 VMin 600 V (+/- 0.125 inch); PLC Code 0; UL 746A
Hot Wire Ignition, HWI30 - 60 sec30 - 60 sec (+/- 0.125 inch); PLC Code 2; UL 746A
High Amp Arc Ignition, HAI60 - 120 arcs60 - 120 arcs Surface (+/- 0.125 inch); PLC Code 1; UL 746A
High Voltage Arc-Tracking Rate, HVTR0 - 10 mm/min0 - 0.394 in/min (+/- 0.125 inch); PLC Code 0; UL 746A

Thermal Properties
CTE, linear 68°F73.8 µm/m-°C41 µin/in-°F Flow, -40F to 100F; ASTM E 831
CTE, linear 68°F, Transverse to Flow70.2 µm/m-°C39 µin/in-°F from -40F to 100F; ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi)132 °C270 °F 0.125 inch, unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi)124 °C255 °F 0.125 inch, unannealed; ASTM D 648
Vicat Softening Point139 °C282 °F Rate B; ASTM D 1525
UL RTI, Electrical130 °C266 °F UL 746B
UL RTI, Mechanical with Impact120 °C248 °F UL 746B
UL RTI, Mechanical without Impact130 °C266 °F UL 746B
Flammability, UL94V-0V-0 0.043 in.

Descriptive Properties
UL File Number, GLOBALE161759 
UL File Number, USAE121562 
Printer friendly version Printer friendly version


Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistant format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

New MatWeb Services

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。