SABIC Innovative Plastics LEXAN 925AU Polycarbonate (North America)
Subcategory: Polycarbonate; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line. MatWeb has a separate entry for the European data sheet.
Physical Properties | Metric | English | Comments |
|
Density | 1.19 g/cc | 0.043 lb/in³ | ASTM D 792 |
Linear Mold Shrinkage | 0.006 - 0.008 cm/cm | 0.006 - 0.008 in/in | Flow, 0.125 inch; ASTM D 955 |
Melt Flow | 13 g/10 min | 13 g/10 min | 300C/1.2 kgf (O); ASTM D 1238 |
Mechanical Properties |
|
Tensile Strength @ Break | 67.6 MPa | 9800 psi | Type I, 2.0 in/min; ASTM D 638 |
Tensile Strength @ Yield | 62.1 MPa | 9000 psi | Type I, 2.0 in/min; ASTM D 638 |
Elongation at Break | 125 % | 125 % | Type I, 2.0 in/min; ASTM D 638 |
Elongation at Yield | 6 % | 6 % | Type I, 2.0 in/min; ASTM D 638 |
Tensile Modulus | 2.28 GPa | 330 ksi | 2.0 in/min; ASTM D 638 |
Flexural Modulus | 2.38 GPa | 345 ksi | 0.05 in/min, 2" span; ASTM D 790 |
Flexural Yield Strength | 101 MPa | 14700 psi | 0.05 in/min, 2" span; ASTM D 790 |
Gardner Impact @ 23°C | 79.1 J | 58.3 ft-lb | Instrumented Impact Total Energy, 73°F; ASTM D 3763 |
Izod Impact, Notched | 8.01 J/cm | 15 ft-lb/in | 73F; ASTM D 256 |
Electrical Properties |
|
Arc Resistance | Max 60 sec | Max 60 sec | Tungsten (+/- 0.125 inch); PLC Code 7; ASTM D 495 |
Comparative Tracking Index | 175 - 250 V | 175 - 250 V | (+/- 0.125 inch); PLC Code 3; UL 746A |
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | (+/- 0.125 inch); PLC Code 2; UL 746A |
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | Surface (+/- 0.125 inch); PLC Code 2; UL 746A |
High Voltage Arc-Tracking Rate, HVTR | 80 - 150 mm/min | 3.15 - 5.91 in/min | (+/- 0.125 inch); PLC Code 3; UL 746A |
Thermal Properties |
|
CTE, linear 68°F | 68.4 µm/m-°C | 38 µin/in-°F | Flow, -40F to 100F; ASTM E 831 |
CTE, linear 68°F, Transverse to Flow | 73.8 µm/m-°C | 41 µin/in-°F | from -40F to 100F; ASTM E 831 |
Deflection Temperature at 0.46 MPa (66 psi) | 138 °C | 280 °F | 0.125 inch, unannealed; ASTM D 648 |
Deflection Temperature at 1.8 MPa (264 psi) | 127 °C | 260 °F | 0.125 inch, unannealed; ASTM D 648 |
Vicat Softening Point | 143 °C | 290 °F | Rate B; ASTM D 1525 |
UL RTI, Electrical | 130 °C | 266 °F | UL 746B |
UL RTI, Mechanical with Impact | 120 °C | 248 °F | UL 746B |
UL RTI, Mechanical without Impact | 130 °C | 266 °F | UL 746B |
Flammability, UL94 | V-2 | V-2 | 0.06 in. |
Flammability, UL94 | V-0 | V-0 | 0.12 in. |
Descriptive Properties | |
UL File Number, USA | E121562 | |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|