SABIC Innovative Plastics LEXAN® 3413 PC, 30% Glass Filler, Flame-Retarded
Subcategory: Filled/Reinforced Thermoplastic; Polycarbonate; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Data provided by GE Plastics. This product grade was removed from GE's database of standard products in 1998.
No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
Physical Properties | Metric | English | Comments |
|
Density | 1.43 g/cc | 0.0517 lb/in³ | ASTM D792 |
Water Absorption | 0.14 % | 0.14 % | 24 hrs at 23°C; ASTM D570 |
Linear Mold Shrinkage | 0.001 - 0.003 cm/cm | 0.001 - 0.003 in/in | at 3.2 mm. |
Mechanical Properties |
|
Tensile Strength, Ultimate | 131 MPa | 19000 psi | ASTM D638 |
Elongation at Break | 3 % | 3 % | ASTM D638 |
Flexural Modulus | 7.579 GPa | 1100 ksi | ASTM D790 |
Flexural Yield Strength | 158 MPa | 22900 psi | ASTM D790 |
Izod Impact, Notched | 1.05 J/cm | 1.97 ft-lb/in | 23°C (73.4°F) |
Electrical Properties |
|
Electrical Resistivity | 1e+017 ohm-cm | 1e+017 ohm-cm | ASTM D257 |
Dielectric Constant | 3.31 | 3.31 | 1 MHz |
Dielectric Constant | 3.35 | 3.35 | 60 Hz |
Dielectric Constant, Low Frequency | 3.35 | 3.35 | 60 Hz |
Dissipation Factor | 0.0011 | 0.0011 | 60 Hz; ASTM D150 |
Dissipation Factor | 0.007 | 0.007 | 1 MHz |
Dissipation Factor, Low Frequency | 0.0011 | 0.0011 | 60 Hz |
Thermal Properties |
|
CTE, linear 20°C | 22 µm/m-°C | 12.2 µin/in-°F | |
Deflection Temperature at 0.46 MPa (66 psi) | 151 °C | 304 °F | ASTM D648 |
Deflection Temperature at 1.8 MPa (264 psi) | 146 °C | 295 °F | ASTM D648 |
Vicat Softening Point | 165 °C | 329 °F | ASTM D1525 |
UL RTI, Electrical | 120 °C | 248 °F | |
UL RTI, Mechanical with Impact | 120 °C | 248 °F | |
UL RTI, Mechanical without Impact | 130 °C | 266 °F | |
Flammability, UL94 | V-1 | V-1 | V-1 UL94 Rating, V-Series at 1.5 mm. |
Processing Properties |
|
Processing Temperature | 315 - 337 °C | 599 - 639 °F | melt temperature |
Mold Temperature | 82 - 115 °C | 180 - 239 °F | |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|