ITW Devcon Rubber Repair / Castable Urethane Flexane® Fast Cure Liquid, Grey
Subcategory: Adhesives, Sealants, and Coatings; Polymer; Polyurethane, TS; Thermoset
Material Notes:
Information provided by ITW Devcon
Physical Properties | Metric | English | Comments |
|
Density | 1.04 g/cc | 0.0377 lb/in³ | |
Viscosity | 5800 cP | 5800 cP | Mixed Viscosity |
Mechanical Properties |
|
Hardness, Shore A | 94 | 94 | Cured; ASTM D2240 |
Tensile Strength @ Break | 22.8 MPa | 3300 psi | ASTM D412 |
Elongation at Break | Max 450 % | Max 450 % | ASTM D412 |
Tear Strength | 75.4 kN/m | 430 pli | ASTM D624 |
Taber Abrasion, mg/1000 Cycles | 330 | 330 | H-18 wheel (1000 gram load) |
Electrical Properties |
|
Dielectric Strength | 13.8 kV/mm | 350 V/mil | ASTM D149 |
Thermal Properties |
|
Maximum Service Temperature, Air | 48.9 °C | 120 °F | wet |
Maximum Service Temperature, Air | 82.2 °C | 180 °F | dry |
Shrinkage | 0.18 % | 0.18 % | Cured; ASTM D2566 |
Processing Properties |
|
Cure Time | 120 min | 2 hour | Functional cure |
Pot Life | 8 min | 8 min | at 75°F |
Descriptive Properties | |
Coverage per pound, in² @ 1/4" thickness | 106 | |
Mix ratio by weight (Resin:Hardener) | 80:20 | |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|