LNP (SABIC Innovative Plastics) LEXAN® BFL2015 Polycarbonate
Subcategory: Polycarbonate; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes:
Information provided by LNP, a GE Plastics Company.
Physical Properties | Metric | English | Comments |
|
Specific Gravity | 1.3 g/cc | 0.047 lb/in³ | ASTM D792 |
Water Absorption | 0.14 % | 0.14 % | at 24 hrs; ASTM D570 |
Linear Mold Shrinkage | 0.0025 - 0.0035 cm/cm | 0.0025 - 0.0035 in/in | 3.20 mm; ASTM D955 |
Mechanical Properties |
|
Tensile Strength, Yield | 84.3 MPa | 12200 psi | ASTM D638 |
Elongation at Break | 4 - 6 % | 4 - 6 % | ASTM D638 |
Flexural Modulus | 4.47 GPa | 648 ksi | ASTM D790 |
Flexural Strength | 133 MPa | 19300 psi | ASTM D790 |
Izod Impact, Notched | 0.91 J/cm | 1.7 ft-lb/in | ASTM D256 |
Thermal Properties |
|
CTE, linear 20°C | 40 - 50 µm/m-°C | 22.2 - 27.8 µin/in-°F | TMA, -30°C to 30°C |
Deflection Temperature at 0.46 MPa (66 psi) | 142 °C | 288 °F | Unannealed (3.20 mm); ASTM D648 |
Flammability, UL94 | V-0 | V-0 | 1.50mm |
|
Printer friendly version |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. Click here to
view all the property values for this datasheet as they were originally entered into MatWeb.
|