RTP Company RTP 1401 L Polyethersulfone (PES) Glass Fiber - Lubricated - UL94 V-0

Return to last searchReturn to last search
Printer friendly version Printer friendly versionAdd to Folder:
Excel Download Download to Excel (requires Excel and Windows)Material suppliers Material suppliers
 Export data to your CAD/FEA program

Subcategory: Polyethersulfone; Polymer; Thermoplastic

Material Notes:
RTP 1401 L is a specially formulated glass fiber reinforced polyethersulfone material that offers improved retention of properties at elevated temperatures and is an excellent material for connectors. It is processible on conventional injection molding equipment.

Click here to view available vendors for this material.

Physical PropertiesMetricEnglishComments
Specific Gravity1.44 g/cc0.052 lb/in³ ASTM D792
Filler Content10 %10 % Primary Additive
Water Absorption0.4 %0.4 % 24 hrs; 23°C; ASTM D570
Linear Mold Shrinkage0.004 - 0.006 cm/cm0.004 - 0.006 in/in 1/8 in (3.2 mm); ASTM D955

Mechanical Properties
Hardness, Rockwell R121121 ASTM D785
Tensile Strength @ Break96.5 MPa14000 psi ASTM D638
Elongation at Break2.5 - 3.5 %2.5 - 3.5 % ASTM D638
Tensile Modulus4.83 GPa700 ksi ASTM D638
Flexural Modulus4.48 GPa650 ksi ASTM D638
Flexural Yield Strength152 MPa22000 psi ASTM D790
Izod Impact, Unnotched5.34 J/cm10 ft-lb/in 1/8 in (3.2 mm); ASTM D4812
Izod Impact, Notched0.374 J/cm0.7 ft-lb/in 1/8 in (3.2 mm); ASTM D256

Electrical Properties
Volume ResistivityMin 1e+016 ohm-cmMin 1e+016 ohm-cm ASTM D257
Dielectric Constant3.73.7 1 MHz; Dry; ASTM D150
Dielectric Strength15 kV/mm380 V/mil S/T; in oil; ASTM D149
Dissipation Factor0.0070.007 1 MHz; Dry; ASTM D150

Thermal Properties
Deflection Temperature at 0.46 MPa (66 psi)207 °C405 °F ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)204 °C400 °F ASTM D648
Flammability, UL94V-0V-0 0.020 in (0.5 mm)

Processing Properties
Melt Temperature343 - 377 °C650 - 710 °F 
Mold Temperature135 - 177 °C275 - 350 °F 
Drying Temperature149 °C300 °F 6 hrs
Moisture Content0.04 %0.04 % 
Dew Point-31.7 °C-25 °F 
Injection Pressure68.9 - 103 MPa10000 - 15000 psi 
Printer friendly version Printer friendly version


Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistant format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Specialty Compounds RTP Company

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。