Antimony Telluride, Sb2Te3


Subcategory: Ceramic; Semiconductor; Sulfide/Chalcogenide

Key Words: Chalcogenide; Semiconductor; Tellurium

Physical PropertiesOriginal ValueComments
Density6.44 g/cc 
a Lattice Constant4.25 Å 
c Lattice Constant30.3 Å 
Molecular Weight626.32 g/mol 

Electrical Properties
Band Gap0.3 eV 
Hole Mobility, cm²/V-s360 

Thermal Properties
Melting Point622 °C 

Descriptive Properties
CAS Number1327-50-0 
ColorGray 
Crystal StructureHexagonal-Rhombohedral Tetradymite Structure - R(-3)M

References are available for this material.

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.