MatWeb, The Online Materials Database
SABIC Innovative Plastics LEXAN EM1210 Polycarbonate (North America)
Subcategory: Polycarbonate; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line.
Physical Properties | Original Value | Comments |
|
Density | 1.19 g/cc | ASTM D 792 |
Water Absorption | 0.16 % | 24 hours @ 73F; ASTM D 570 |
Linear Mold Shrinkage | 0.005 - 0.007 cm/cm | Flow, 0.125 inch; ASTM D 955 |
Melt Flow | 13 g/10 min | 300C/1.2 kgf (O); ASTM D 1238 |
Mechanical Properties |
|
Tensile Strength @ Yield | 8300 psi | Type I, 2.0 in/min; ASTM D 638 |
Elongation at Break | 110 % | Type I, 2.0 in/min; ASTM D 638 |
Flexural Modulus | 295000 psi | 0.05 in/min, 2" span; ASTM D 790 |
Flexural Yield Strength | 11800 psi | 0.05 in/min, 2" span; ASTM D 790 |
Izod Impact, Notched, Low Temp | 13 ft-lb/in | at -22F; ASTM D 256 |
Gardner Impact @ 23°C | 540 in-lb | Instrumented Impact Energy @ peak, 73F; ASTM D 3763 |
Gardner Impact @ 23°C | 580 in-lb | Instrumented Impact Energy @ peak, -22°F; ASTM D 3763 |
Izod Impact, Notched | 13 ft-lb/in | 73F, 0.250"; ASTM D 256 |
Izod Impact, Notched | 14.5 ft-lb/in | 73F; ASTM D 256 |
Thermal Properties |
|
CTE, linear 68°F | 36 µin/in-°F | Flow, -40F to 200F; ASTM E 831 |
Deflection Temperature at 0.46 MPa (66 psi) | 275 °F | 0.250 inch, unannealed; ASTM D 648 |
Deflection Temperature at 1.8 MPa (264 psi) | 262 °F | 0.250 inch, unannealed; ASTM D 648 |
|
|
|
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
|