MatWeb, The Online Materials Database
SABIC Innovative Plastics LEXAN EM2212 Polycarbonate (North America)
Subcategory: Polycarbonate; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line.
Physical Properties | Original Value | Comments |
|
Density | 1.24 g/cc | ASTM D 792 |
Water Absorption | 0.14 % | 24 hours @ 73F; ASTM D 570 |
Linear Mold Shrinkage | 0.003 - 0.005 cm/cm | Flow, 0.125 inch; ASTM D 955 |
Mechanical Properties |
|
Tensile Strength @ Break | 8200 psi | Type I, 0.2 in/min; ASTM D 638 |
Elongation at Break | 14 % | Type I, 0.2 in/min; ASTM D 638 |
Flexural Modulus | 400000 psi | 0.05 in/min, 2" span; ASTM D 790 |
Flexural Yield Strength | 13600 psi | 0.05 in/min, 2" span; ASTM D 790 |
Izod Impact, Notched, Low Temp | 3 ft-lb/in | at -22F; ASTM D 256 |
Gardner Impact @ 23°C | 220 in-lb | Instrumented Impact Energy @ peak, 73F; ASTM D 3763 |
Izod Impact, Notched | 2.5 ft-lb/in | 73F, 0.250"; ASTM D 256 |
Izod Impact, Notched | 4 ft-lb/in | 73F; ASTM D 256 |
Thermal Properties |
|
CTE, linear 68°F | 20 µin/in-°F | Flow, -40F to 200F; ASTM E 831 |
Deflection Temperature at 0.46 MPa (66 psi) | 280 °F | 0.250 inch, unannealed; ASTM D 648 |
Deflection Temperature at 1.8 MPa (264 psi) | 270 °F | 0.250 inch, unannealed; ASTM D 648 |
UL RTI, Electrical | 80 °C | UL 746B |
UL RTI, Mechanical with Impact | 80 °C | UL 746B |
UL RTI, Mechanical without Impact | 80 °C | UL 746B |
Flammability, UL94 | HB | 0.059 in. |
Descriptive Properties | |
UL File Number, USA | E121562 | |
|
|
|
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
|