SABIC Innovative Plastics LEXAN FL3000 Polycarbonate (North America)
Subcategory: Polycarbonate; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line.
Physical Properties | Metric | English | Comments |
|
Density | 1.07 g/cc | 0.0387 lb/in³ | Molded Foam; ASTM D 792 |
Density | 1.19 g/cc | 0.043 lb/in³ | ASTM D 792 |
Linear Mold Shrinkage | 0.009 - 0.011 cm/cm | 0.009 - 0.011 in/in | Flow, 0.250 inch; ASTM D 955 |
Melt Flow | 9.5 g/10 min | 9.5 g/10 min | 300C/1.2 kgf (O); ASTM D 1238 |
Mechanical Properties |
|
Tensile Strength @ Break | 40.7 MPa | 5900 psi | 0.250"; ASTM D 638 |
Elongation at Break | 3.2 % | 3.2 % | 0.250"; ASTM D 638 |
Tensile Modulus | 2.82 GPa | 409 ksi | 0.250"; ASTM D 638 |
Flexural Modulus | 1.9 GPa | 275 ksi | 0.250"; ASTM D 790 |
Flexural Yield Strength | 72.4 MPa | 10500 psi | 0.250"; ASTM D 790 |
Izod Impact, Unnotched | 9.08 J/cm | 17 ft-lb/in | 73F, 0.250"; ASTM D 4812 |
Gardner Impact @ 23°C | 89.5 J | 66 ft-lb | Instrumented Impact Total Energy, 73°F; ASTM D 3763 |
Gardner Impact @ 23°C | 94.9 J | 70 ft-lb | Instrumented Impact Total Energy, 0F; ASTM D 3763 |
Gardner Impact @ 23°C | 94.9 J | 70 ft-lb | Instrumented Impact Total Energy, -40F; ASTM D 3673 |
Thermal Properties |
|
Deflection Temperature at 0.46 MPa (66 psi) | 131 °C | 268 °F | 0.250 inch, unannealed; ASTM D 648 |
Deflection Temperature at 1.8 MPa (264 psi) | 120 °C | 248 °F | 0.250 inch, unannealed; ASTM D 648 |
UL RTI, Electrical | 50 °C | 122 °F | UL 746B |
UL RTI, Mechanical with Impact | 50 °C | 122 °F | UL 746B |
UL RTI, Mechanical without Impact | 50 °C | 122 °F | UL 746B |
Flammability, UL94 | V-0 | V-0 | 0.118 in. |
Flammability, UL94 | 7 | 7 | 0.24 in. |
Flammability Test | 1.07 | 1.07 | FOAM - Flame Class Minimum Density; g/cm3 |
Descriptive Properties | |
Foam Weight Reduction | 10% | Mechanical Properties Reported Herein (0.250") |
Foam Weight Reduction | 10% | Impact Properties Reported Herein (0.250") |
Foam Weight Reduction | 10% | Thermal Properties Reported Herein (0.250") |
Foam Weight Reduction | 10% | Physical Properties Reported Herein (0.250") |
UL File Number, USA | E121562 | |
UV-light, water exposure/immersion | F1 | UL746C |
|
|
|
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
|