SABIC Innovative Plastics LEXAN FXL171R Polycarbonate (North America)
Subcategory: Polycarbonate; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line. MatWeb has a separate entry for the European data sheet.
Physical Properties | Original Value | Comments |
|
Density | 1.2 g/cc | ASTM D 792 |
Linear Mold Shrinkage | 0.006 - 0.008 cm/cm | Flow, 0.125 inch; ASTM D 955 |
Melt Flow | 25 g/10 min | 300C/1.2 kgf (O); ASTM D 1238 |
Mechanical Properties |
|
Tensile Strength @ Break | 9300 psi | Type I, 2.0 in/min; ASTM D 638 |
Tensile Strength @ Yield | 9000 psi | Type I, 2.0 in/min; ASTM D 638 |
Elongation at Break | 125 % | Type I, 2.0 in/min; ASTM D 638 |
Elongation at Yield | 6.2 % | Type I, 2.0 in/min; ASTM D 638 |
Tensile Modulus | 338000 psi | 2.0 in/min; ASTM D 638 |
Flexural Modulus | 340000 psi | 0.05 in/min, 2" span; ASTM D 790 |
Flexural Yield Strength | 13500 psi | 0.05 in/min, 2" span; ASTM D 790 |
Gardner Impact @ 23°C | 620 in-lb | Instrumented Impact Total Energy, 73°F; ASTM D 3763 |
Izod Impact, Notched | 14.6 ft-lb/in | 73F; ASTM D 256 |
Thermal Properties |
|
Deflection Temperature at 0.46 MPa (66 psi) | 280 °F | 0.125 inch, unannealed; ASTM D 648 |
Deflection Temperature at 1.8 MPa (264 psi) | 260 °F | 0.125 inch, unannealed; ASTM D 648 |
|
|
|
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
|