Physical Properties | Metric | English | Comments |
|
Density | 1.2 g/cc | 0.0434 lb/in³ | ASTM D 792 |
Water Absorption | 0.1 % | 0.1 % | 24 hours @ 73F; ASTM D 570 |
Water Absorption at Saturation | 0.35 % | 0.35 % | Equilibrium, 73F; ASTM D 570 |
Water Absorption at Saturation | 0.58 % | 0.58 % | Equilibrium, 212F; ASTM D 570 |
Linear Mold Shrinkage | 0.005 - 0.007 cm/cm | 0.005 - 0.007 in/in | Flow, 0.125 inch; ASTM D 955 |
Melt Flow | 25 g/10 min | 25 g/10 min | 300C/1.2 kgf (O); ASTM D 1238 |
Mechanical Properties |
|
Tensile Strength @ Break | 65.5 MPa | 9500 psi | Type I, 2.0 in/min; ASTM D 638 |
Tensile Strength @ Yield | 62.1 MPa | 9000 psi | Type I, 2.0 in/min; ASTM D 638 |
Elongation at Break | 120 % | 120 % | Type I, 2.0 in/min; ASTM D 638 |
Flexural Modulus | 2.31 GPa | 335 ksi | 0.05 in/min, 2" span; ASTM D 790 |
Flexural Yield Strength | 93.1 MPa | 13500 psi | 0.05 in/min, 2" span; ASTM D 790 |
Gardner Impact @ 23°C | 54.2 J | 40 ft-lb | Instrumented Impact Energy @ peak, 73F; ASTM D 3763 |
Tensile Impact Strength | 378 kJ/m² | 180 ft-lb/in² | Type "S"; ASTM D 1822 |
Izod Impact, Notched | 6.41 J/cm | 12 ft-lb/in | 73F; ASTM D 256 |
Electrical Properties |
|
Comparative Tracking Index | 250 - 400 V | 250 - 400 V | (+/- 0.125 inch); PLC Code 2; UL 746A |
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | (+/- 0.125 inch); PLC Code 2; UL 746A |
High Amp Arc Ignition, HAI | 60 - 120 arcs | 60 - 120 arcs | Surface (+/- 0.125 inch); PLC Code 1; UL 746A |
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80 mm/min | 1 - 3.15 in/min | (+/- 0.125 inch); PLC Code 2; UL 746A |
Thermal Properties |
|
Deflection Temperature at 1.8 MPa (264 psi) | 127 °C | 260 °F | 0.125 inch, unannealed; ASTM D 648 |
UL RTI, Electrical | 130 °C | 266 °F | UL 746B |
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746B |
UL RTI, Mechanical without Impact | 130 °C | 266 °F | UL 746B |
Flammability, UL94 | V-2 | V-2 | 0.043 in. |
Optical Properties |
|
Haze | 1 % | 1 % | 0.100 inch; ASTM D 1003 |
Transmission, Visible | 88 % | 88 % | 0.100 inch; ASTM D 1003 |
Descriptive Properties |
|
CSA File No. | LS88480 | |
UL File Number, USA | E121562 | |