MatWeb, The Online Materials Database
SABIC Innovative Plastics LEXAN LS1 Polycarbonate (North America)
Subcategory: Polycarbonate; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line. MatWeb has a separate entry for the European data sheet.
Physical Properties | Metric | English | Comments |
|
Density | 1.2 g/cc | 0.0434 lb/in³ | ASTM D 792 |
Water Absorption | 0.15 % | 0.15 % | 24 hours @ 73F; ASTM D 570 |
Linear Mold Shrinkage | 0.005 - 0.007 cm/cm | 0.005 - 0.007 in/in | Flow, 0.125 inch; ASTM D 955 |
Melt Flow | 17.5 g/10 min | 17.5 g/10 min | 300C/1.2 kgf (O); ASTM D 1238 |
Mechanical Properties |
|
Tensile Strength @ Yield | 62.1 MPa | 9000 psi | Type I, 2.0 in/min; ASTM D 638 |
Elongation at Break | 125 % | 125 % | Type I, 2.0 in/min; ASTM D 638 |
Flexural Modulus | 2.34 GPa | 340 ksi | 0.05 in/min, 2" span; ASTM D 790 |
Flexural Yield Strength | 96.5 MPa | 14000 psi | 0.05 in/min, 2" span; ASTM D 790 |
Gardner Impact @ 23°C | 62.1 J | 45.8 ft-lb | Instrumented Impact Energy @ peak, 73F; ASTM D 3763 |
Tensile Impact Strength | 472 kJ/m² | 225 ft-lb/in² | Type "S"; ASTM D 1822 |
Falling Dart Impact | 169 J | 125 ft-lb | 73F; GE Test |
Izod Impact, Notched | 6.94 J/cm | 13 ft-lb/in | 73F; ASTM D 256 |
Electrical Properties |
|
Comparative Tracking Index | 250 - 400 V | 250 - 400 V | (+/- 0.125 inch); PLC Code 2; UL 746A |
Hot Wire Ignition, HWI | 7 - 15 sec | 7 - 15 sec | (+/- 0.125 inch); PLC Code 4; UL 746A |
High Amp Arc Ignition, HAI | 60 - 120 arcs | 60 - 120 arcs | Surface (+/- 0.125 inch); PLC Code 1; UL 746A |
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80 mm/min | 1 - 3.15 in/min | (+/- 0.125 inch); PLC Code 2; UL 746A |
Thermal Properties |
|
Deflection Temperature at 1.8 MPa (264 psi) | 129 °C | 265 °F | 0.250 inch, unannealed; ASTM D 648 |
UL RTI, Electrical | 100 °C | 212 °F | UL 746B |
UL RTI, Mechanical with Impact | 100 °C | 212 °F | UL 746B |
UL RTI, Mechanical without Impact | 100 °C | 212 °F | UL 746B |
Flammability, UL94 | HB | HB | 0.058 in. |
Optical Properties |
|
Transmission, Visible | 88 % | 88 % | 0.100 inch; ASTM D 1003 |
Descriptive Properties | |
UL File Number, USA | E121562 | |
UV-light, water exposure/immersion | F1 | UL746C |
|
|
|
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
|