SABIC Innovative Plastics LEXAN ML4189 Polycarbonate (North America)
Subcategory: Polycarbonate; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line.
Physical Properties | Original Value | Comments |
|
Density | 1.2 g/cc | ASTM D 792 |
Water Absorption | 0.15 % | 24 hours @ 73F; ASTM D 570 |
Melt Flow | 13.5 g/10 min | 300C/1.2 kgf (O); ASTM D 1238 |
Mechanical Properties |
|
Tensile Strength @ Yield | 9000 psi | Type I, 2.0 in/min; ASTM D 638 |
Elongation at Break | 110 % | Type I, 2.0 in/min; ASTM D 638 |
Flexural Modulus | 340000 psi | 0.05 in/min, 2" span; ASTM D 790 |
Flexural Yield Strength | 13500 psi | 0.05 in/min, 2" span; ASTM D 790 |
Tensile Impact Strength | 262 ft-lb/in² | Type "S"; ASTM D 1822 |
Falling Dart Impact | 125 ft-lb | 73F; ASTM D 3029 |
Izod Impact, Notched | 14 ft-lb/in | 73F; ASTM D 256 |
Electrical Properties |
|
Dielectric Strength | 380 V/mil | in air, 125 mils; ASTM D 149 |
Comparative Tracking Index | 250 - 400 V | (+/- 0.125 inch); PLC Code 2; UL 746A |
Hot Wire Ignition, HWI | 30 - 60 sec | (+/- 0.125 inch); PLC Code 2; UL 746A |
High Amp Arc Ignition, HAI | 60 - 120 arcs | Surface (+/- 0.125 inch); PLC Code 1; UL 746A |
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80 mm/min | (+/- 0.125 inch); PLC Code 2; UL 746A |
Thermal Properties |
|
Deflection Temperature at 1.8 MPa (264 psi) | 262 °F | 0.250 inch, unannealed; ASTM D 648 |
UL RTI, Electrical | 130 °C | UL 746B |
UL RTI, Mechanical with Impact | 130 °C | UL 746B |
UL RTI, Mechanical without Impact | 130 °C | UL 746B |
Flammability, UL94 | V-2 | 0.043 in. |
Flammability, UL94 | V-0 | 0.236 in. |
Oxygen Index | 25 % | ASTM D 2863 |
Optical Properties |
|
Transmission, Visible | 87.5 % | 0.100 inch; ASTM D 1003 |
Descriptive Properties | |
UL File Number, USA | E121562 | |
UV-light, water exposure/immersion | F2 | UL746C |
|
|
|
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
|