SABIC Innovative Plastics LEXAN ML6339R Polycarbonate (North America)
Subcategory: Polycarbonate; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line.
Physical Properties | Metric | English | Comments |
|
Density | 1.17 g/cc | 0.0423 lb/in³ | ASTM D 792 |
Water Absorption | 0.13 % | 0.13 % | 24 hours @ 73F; ASTM D 570 |
Water Absorption at Saturation | 0.3 % | 0.3 % | Equilibrium, 73F; ASTM D 570 |
Linear Mold Shrinkage | 0.005 - 0.007 cm/cm | 0.005 - 0.007 in/in | Flow, 0.125 inch; ASTM D 955 |
Melt Flow | 10 g/10 min | 10 g/10 min | 300C/1.2 kgf (O); ASTM D 1238 |
Mechanical Properties |
|
Tensile Strength @ Break | 53.1 MPa | 7700 psi | Type I, 2.0 in/min; ASTM D 638 |
Tensile Strength @ Yield | 57.9 MPa | 8400 psi | Type I, 2.0 in/min; ASTM D 638 |
Elongation at Break | 120 % | 120 % | Type I, 2.0 in/min; ASTM D 638 |
Flexural Modulus | 1.93 GPa | 280 ksi | 0.05 in/min, 2" span; ASTM D 790 |
Flexural Yield Strength | 77.9 MPa | 11300 psi | 0.05 in/min, 2" span; ASTM D 790 |
Izod Impact, Notched, Low Temp | 5.87 J/cm | 11 ft-lb/in | at -22F; ASTM D 256 |
Gardner Impact @ 23°C | 61 J | 45 ft-lb | Instrumented Impact Total Energy, 73°F; ASTM D 3763 |
Gardner Impact @ 23°C | 70.3 J | 51.8 ft-lb | Instrumented Impact Energy @ peak, 73F; ASTM D 3763 |
Izod Impact, Notched | 6.41 J/cm | 12 ft-lb/in | 73F, 0.250"; ASTM D 256 |
Izod Impact, Notched | 8.01 J/cm | 15 ft-lb/in | 73F; ASTM D 256 |
Electrical Properties |
|
Comparative Tracking Index | 250 - 400 V | 250 - 400 V | (+/- 0.125 inch); PLC Code 2; UL 746A |
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | (+/- 0.125 inch); PLC Code 2; UL 746A |
High Amp Arc Ignition, HAI | Min 120 arcs | Min 120 arcs | Surface (+/- 0.125 inch); PLC Code 0; UL 746A |
Thermal Properties |
|
Deflection Temperature at 1.8 MPa (264 psi) | 106 °C | 222 °F | 0.125 inch, unannealed; ASTM D 648 |
Deflection Temperature at 1.8 MPa (264 psi) | 111 °C | 231 °F | 0.250 inch, unannealed; ASTM D 648 |
UL RTI, Electrical | 80 °C | 176 °F | UL 746B |
UL RTI, Mechanical with Impact | 80 °C | 176 °F | UL 746B |
UL RTI, Mechanical without Impact | 80 °C | 176 °F | UL 746B |
Flammability, UL94 | HB | HB | 0.043 in. |
Descriptive Properties | |
UL File Number, USA | E121562 | |
|
|
|
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
|