SABIC Innovative Plastics LEXAN ML6451 Polycarbonate (North America)


Subcategory: Polycarbonate; Polymer; Thermoplastic

Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.

Material Notes:
Information provided by GE Plastics for their North American product line.

Physical PropertiesOriginal ValueComments
Density1.19 g/cc ASTM D 792
Melt Flow10.5 g/10 min 300C/1.2 kgf (O); ASTM D 1238

Mechanical Properties
Tensile Strength @ Break10530 psi Type I, 2.0 in/min; ASTM D 638
Tensile Strength @ Yield10330 psi Type I, 2.0 in/min; ASTM D 638
Elongation at Break98 % Type I, 2.0 in/min; ASTM D 638
Flexural Modulus377000 psi 0.05 in/min, 2" span; ASTM D 790
Flexural Yield Strength15200 psi 0.05 in/min, 2" span; ASTM D 790
Izod Impact, Notched1.7 ft-lb/in 73F; ASTM D 256

Thermal Properties
Deflection Temperature at 1.8 MPa (264 psi)238 °F 0.125 inch, unannealed; ASTM D 648

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.