SABIC Innovative Plastics LEXAN OQ4620 Polycarbonate (North America)


Subcategory: Polycarbonate; Polymer; Thermoplastic

Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.

Material Notes:
Information provided by GE Plastics for their North American product line.

Physical PropertiesOriginal ValueComments
Density1.2 g/cc ASTM D 792
Linear Mold Shrinkage0.005 - 0.007 cm/cm Flow, 0.125 inch; ASTM D 955
Melt Flow8.5 g/10 min 300C/1.2 kgf (O); ASTM D 1238

Mechanical Properties
Tensile Strength @ Yield9000 psi Type I, 2.0 in/min; ASTM D 638
Elongation at Yield130 % Type I, 2.0 in/min; ASTM D 638
Flexural Modulus340000 psi 0.05 in/min, 2" span; ASTM D 790
Flexural Yield Strength14200 psi 0.05 in/min, 2" span; ASTM D 790
Falling Dart Impact125 ft-lb 73F; ASTM D 3029
Izod Impact, Notched14 ft-lb/in 73F; ASTM D 256

Thermal Properties
Deflection Temperature at 1.8 MPa (264 psi)270 °F 0.250 inch, unannealed; ASTM D 648

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.