Physical PropertiesOriginal ValueComments
Density1.2 g/cc ASTM D 792
Melt Flow7 g/10 min 300C/1.2 kgf (O); ASTM D 1238

Mechanical Properties
Tensile Strength @ Break9500 psi Type I, 2.0 in/min; ASTM D 638
Tensile Strength @ Yield9000 psi Type I, 2.0 in/min; ASTM D 638
Flexural Modulus340000 psi 0.05 in/min, 2" span; ASTM D 790
Flexural Yield Strength13500 psi 0.05 in/min, 2" span; ASTM D 790
Izod Impact, Notched14 ft-lb/in 73F; ASTM D 256

Thermal Properties
Deflection Temperature at 0.46 MPa (66 psi)280 °F 0.250 inch, unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi)270 °F 0.250 inch, unannealed; ASTM D 648
Vicat Softening Point310 °F Rate B; ASTM D 1525

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.