MatWeb, The Online Materials Database
SABIC Innovative Plastics LEXAN 3412HF Polycarbonate (North America)
Subcategory: Polycarbonate; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line.
Physical Properties | Original Value | Comments |
|
Density | 1.34 g/cc | ASTM D 792 |
Linear Mold Shrinkage | 0.002 - 0.004 cm/cm | Flow, 0.125 inch; ASTM D 955 |
Linear Mold Shrinkage, Transverse | 0.0045 - 0.0065 cm/cm | 0.125 inch; ASTM D 955 |
Melt Flow | 8.5 g/10 min | 300C/1.2 kgf (O); ASTM D 1238 |
Mechanical Properties |
|
Tensile Strength @ Break | 15500 psi | Type I, 0.2 in/min; ASTM D 638 |
Tensile Strength @ Yield | 14500 psi | Type I, 0.2 in/min; ASTM D 638 |
Elongation at Break | 4 % | Type I, 0.2 in/min; ASTM D 638 |
Tensile Modulus | 500000 psi | 0.2 in/min; ASTM D 638 |
Flexural Modulus | 800000 psi | 0.05 in/min, 2" span; ASTM D 790 |
Flexural Strength | 24000 psi | 0.05 in/min, 2" span; ASTM D 790 |
Flexural Yield Strength | 22700 psi | 0.05 in/min, 2" span; ASTM D 790 |
Izod Impact, Unnotched | 10 ft-lb/in | 73F; ASTM D 4812 |
Gardner Impact @ 23°C | 30 in-lb | Instrumented Impact Total Energy, 73°F; ASTM D 3763 |
Izod Impact, Notched | 2 ft-lb/in | 73F; ASTM D 256 |
Thermal Properties |
|
Deflection Temperature at 0.46 MPa (66 psi) | 287 °F | 0.125 inch, unannealed; ASTM D 648 |
Deflection Temperature at 1.8 MPa (264 psi) | 280 °F | 0.125 inch, unannealed; ASTM D 648 |
UL RTI, Electrical | 80 °C | UL 746B |
UL RTI, Mechanical with Impact | 80 °C | UL 746B |
UL RTI, Mechanical without Impact | 80 °C | UL 746B |
Flammability, UL94 | V-1 | 0.059 in. |
Flammability, UL94 | V-0 | 0.118 in. |
Descriptive Properties | |
UL File Number, USA | E121562 | |
|
|
|
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
|