MatWeb, The Online Materials Database
SABIC Innovative Plastics LEXAN 4501 Polycarbonate (North America)
Subcategory: Polycarbonate; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line.
Physical Properties | Original Value | Comments |
|
Density | 1.2 g/cc | ASTM D 792 |
Water Absorption | 0.16 % | 24 hours @ 73F; ASTM D 570 |
Linear Mold Shrinkage | 0.007 - 0.008 cm/cm | Flow, 0.125 inch; ASTM D 955 |
Melt Flow | 3 g/10 min | 300C/1.2 kgf (O); ASTM D 1238 |
Mechanical Properties |
|
Hardness, Rockwell M | 85 | ASTM D 785 |
Hardness, Rockwell R | 122 | ASTM D 785 |
Tensile Strength @ Break | 10400 psi | Type I, 2.0 in/min; ASTM D 638 |
Tensile Strength @ Yield | 9500 psi | Type I, 2.0 in/min; ASTM D 638 |
Elongation at Break | 122 % | Type I, 2.0 in/min; ASTM D 638 |
Flexural Modulus | 294000 psi | 0.05 in/min, 2" span; ASTM D 790 |
Flexural Yield Strength | 13800 psi | 0.05 in/min, 2" span; ASTM D 790 |
Izod Impact, Unnotched | 60 ft-lb/in | 73F; ASTM D 4812 |
Tensile Impact Strength | 275 ft-lb/in² | Type "S"; ASTM D 1822 |
Falling Dart Impact | 110 ft-lb | 73F; ASTM D 3029 |
Izod Impact, Notched | 12 ft-lb/in | 73F; ASTM D 256 |
Electrical Properties |
|
Volume Resistivity | Min 2.6e+016 ohm-cm | ASTM D 257 |
Dielectric Constant | 3 | 1 MHz; ASTM D 150 |
Dielectric Constant | 3.15 | 60 Hz; ASTM D 150 |
Dielectric Strength | 515 V/mil | in air, 125 mils; ASTM D 149 |
Dissipation Factor | 0.0012 | 60 Hz; ASTM D 150 |
Dissipation Factor | 0.024 | 100 Hz; ASTM D 150 |
Comparative Tracking Index | 175 - 250 V | (+/- 0.125 inch); PLC Code 3; UL 746A |
Hot Wire Ignition, HWI | 30 - 60 sec | (+/- 0.125 inch); PLC Code 2; UL 746A |
High Amp Arc Ignition, HAI | Max 15 arcs | Surface (+/- 0.125 inch); PLC Code 4; UL 746A |
High Voltage Arc-Tracking Rate, HVTR | 80 - 150 mm/min | (+/- 0.125 inch); PLC Code 3; UL 746A |
Thermal Properties |
|
CTE, linear 68°F | 51 µin/in-°F | Flow, -40F to 200F; ASTM E 831 |
Specific Heat Capacity | 0.3 BTU/lb-°F | ASTM C 351 |
Thermal Conductivity | 0.21 W/m-K | ASTM C 177 |
Deflection Temperature at 1.8 MPa (264 psi) | 290 °F | 0.125 inch, unannealed; ASTM D 648 |
UL RTI, Electrical | 125 °C | UL 746B |
UL RTI, Mechanical with Impact | 125 °C | UL 746B |
UL RTI, Mechanical without Impact | 125 °C | UL 746B |
Flammability, UL94 | V-2 | 0.058 in. |
Optical Properties |
|
Refractive Index | 1.6 | ASTM D 542 |
Haze | 1 % | 0.100 inch; ASTM D 1003 |
Transmission, Visible | 85 % | 0.100 inch; ASTM D 1003 |
Descriptive Properties | |
UL File Number, USA | E121562 | |
|
|
|
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
|