Physical Properties | Metric | English | Comments |
|
Density | 1.21 g/cc | 0.0437 lb/in³ | ASTM D 792 |
Water Absorption | 0.15 % | 0.15 % | 24 hours @ 73F; ASTM D 570 |
Water Absorption at Saturation | 0.35 % | 0.35 % | Equilibrium, 73F; ASTM D 570 |
Water Absorption at Saturation | 0.58 % | 0.58 % | Equilibrium, 212F; ASTM D 570 |
Linear Mold Shrinkage | 0.005 - 0.007 cm/cm | 0.005 - 0.007 in/in | Flow, 0.125 inch; ASTM D 955 |
Melt Flow | 14.5 g/10 min | 14.5 g/10 min | 300C/1.2 kgf (O); ASTM D 1238 |
Mechanical Properties |
|
Hardness, Rockwell M | 70 | 70 | ASTM D 785 |
Hardness, Rockwell R | 118 | 118 | ASTM D 785 |
Tensile Strength @ Break | 55.8 MPa | 8100 psi | Type I, 2.0 in/min; ASTM D 638 |
Tensile Strength @ Yield | 62.1 MPa | 9000 psi | Type I, 2.0 in/min; ASTM D 638 |
Elongation at Break | 90 % | 90 % | Type I, 2.0 in/min; ASTM D 638 |
Elongation at Yield | 7 % | 7 % | Type I, 2.0 in/min; ASTM D 638 |
Flexural Modulus | 2.24 GPa | 325 ksi | 0.05 in/min, 2" span; ASTM D 790 |
Flexural Yield Strength | 91 MPa | 13200 psi | 0.05 in/min, 2" span; ASTM D 790 |
Fatigue Strength | 6.89 MPa | 1000 psi | Fatigue Limit, 2.5 MM cycles; ASTM D 671 |
Izod Impact, Unnotched | 32 J/cm | 60 ft-lb/in | 73F; ASTM D 4812 |
Tensile Impact Strength | 525 kJ/m² | 250 ft-lb/in² | Type "S"; ASTM D 1822 |
Falling Dart Impact | 169 J | 125 ft-lb | 73F; ASTM D 3029 |
Taber Abrasion, mg/1000 Cycles | 10 | 10 | CS-17, 1 kg; ASTM D 1044 |
Izod Impact, Notched | 6.41 J/cm | 12 ft-lb/in | 73F; ASTM D 256 |
Electrical Properties |
|
Volume Resistivity | Min 1e+017 ohm-cm | Min 1e+017 ohm-cm | ASTM D 257 |
Dielectric Constant | 2.96 | 2.96 | 1 MHz; ASTM D 150 |
Dielectric Constant | 3.01 | 3.01 | 60 Hz; ASTM D 150 |
Dielectric Strength | 16.7 kV/mm | 425 V/mil | in air, 125 mils; ASTM D 149 |
Dissipation Factor | 0.0009 | 0.0009 | 60 Hz; ASTM D 150 |
Dissipation Factor | 0.01 | 0.01 | 1 MHz; ASTM D 150 |
Arc Resistance | Max 60 sec | Max 60 sec | Tungsten (+/- 0.125 inch); PLC Code 7; ASTM D 495 |
Comparative Tracking Index | 250 - 400 V | 250 - 400 V | (+/- 0.125 inch); PLC Code 2; UL 746A |
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | (+/- 0.125 inch); PLC Code 2; UL 746A |
High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | Surface (+/- 0.125 inch); PLC Code 3; UL 746A |
High Voltage Arc-Tracking Rate, HVTR | Min 150 mm/min | Min 5.91 in/min | (+/- 0.125 inch); PLC Code 4; UL 746A |
Thermal Properties |
|
CTE, linear 68°F | 68.4 µm/m-°C | 38 µin/in-°F | Flow, -40F to 200F; ASTM E 831 |
Thermal Conductivity | 0.19 W/m-K | 1.32 BTU-in/hr-ft²-°F | ASTM C 177 |
Deflection Temperature at 0.46 MPa (66 psi) | 138 °C | 280 °F | 0.250 inch, unannealed; ASTM D 648 |
Deflection Temperature at 1.8 MPa (264 psi) | 132 °C | 270 °F | 0.250 inch, unannealed; ASTM D 648 |
Vicat Softening Point | 152 °C | 305 °F | Rate B; ASTM D 1525 |
UL RTI, Electrical | 130 °C | 266 °F | UL 746B |
UL RTI, Mechanical with Impact | 120 °C | 248 °F | UL 746B |
UL RTI, Mechanical without Impact | 130 °C | 266 °F | UL 746B |
Flammability, UL94 | V-0 | V-0 | 0.058 in. |
Oxygen Index | 35 % | 35 % | ASTM D 2863 |
Descriptive Properties |
|
CSA File No. | LS88480 | |
UL File Number, USA | E121562 | |
UV-light, water exposure/immersion | F1 | UL746C |