SABIC Innovative Plastics LEXAN 950ASR Polycarbonate (North America)


Subcategory: Polycarbonate; Polymer; Thermoplastic

Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.

Material Notes:
Information provided by GE Plastics for their North American product line.

Physical PropertiesMetricEnglishComments
Density1.21 g/cc0.0437 lb/in³ ASTM D 792
Water Absorption0.15 %0.15 % 24 hours @ 73F; ASTM D 570
Water Absorption at Saturation0.35 %0.35 % Equilibrium, 73F; ASTM D 570
Water Absorption at Saturation0.58 %0.58 % Equilibrium, 212F; ASTM D 570
Linear Mold Shrinkage0.005 - 0.007 cm/cm0.005 - 0.007 in/in Flow, 0.125 inch; ASTM D 955
Melt Flow7 g/10 min7 g/10 min 300C/1.2 kgf (O); ASTM D 1238

Mechanical Properties
Hardness, Rockwell M7070 ASTM D 785
Hardness, Rockwell R118118 ASTM D 785
Tensile Strength @ Break55.8 MPa8100 psi Type I, 2.0 in/min; ASTM D 638
Tensile Strength @ Yield62.1 MPa9000 psi Type I, 2.0 in/min; ASTM D 638
Elongation at Break90 %90 % Type I, 2.0 in/min; ASTM D 638
Elongation at Yield7 %7 % Type I, 2.0 in/min; ASTM D 638
Flexural Modulus2.24 GPa325 ksi 0.05 in/min, 2" span; ASTM D 790
Flexural Yield Strength91 MPa13200 psi 0.05 in/min, 2" span; ASTM D 790
Fatigue Strength6.89 MPa1000 psi Fatigue Limit, 2.5 MM cycles; ASTM D 671
Izod Impact, Unnotched32 J/cm60 ft-lb/in 73F; ASTM D 4812
Tensile Impact Strength525 kJ/m²250 ft-lb/in² Type "S"; ASTM D 1822
Falling Dart Impact169 J125 ft-lb 73F; ASTM D 3029
Taber Abrasion, mg/1000 Cycles1010 CS-17, 1 kg; ASTM D 1044
Izod Impact, Notched6.41 J/cm12 ft-lb/in 73F; ASTM D 256

Electrical Properties
Volume ResistivityMin 1e+017 ohm-cmMin 1e+017 ohm-cm ASTM D 257
Dielectric Constant2.962.96 1 MHz; ASTM D 150
Dielectric Constant3.013.01 60 Hz; ASTM D 150
Dielectric Strength16.7 kV/mm425 V/mil in air, 125 mils; ASTM D 149
Dissipation Factor0.00090.0009 60 Hz; ASTM D 150
Dissipation Factor0.010.01 1 MHz; ASTM D 150
Arc ResistanceMax 60 secMax 60 sec Tungsten (+/- 0.125 inch); PLC Code 7; ASTM D 495
Comparative Tracking Index250 - 400 V250 - 400 V (+/- 0.125 inch); PLC Code 2; UL 746A
Hot Wire Ignition, HWI30 - 60 sec30 - 60 sec (+/- 0.125 inch); PLC Code 2; UL 746A
High Amp Arc Ignition, HAI15 - 30 arcs15 - 30 arcs Surface (+/- 0.125 inch); PLC Code 3; UL 746A
High Voltage Arc-Tracking Rate, HVTR80 - 150 mm/min3.15 - 5.91 in/min (+/- 0.125 inch); PLC Code 3; UL 746A

Thermal Properties
CTE, linear 68°F68.4 µm/m-°C38 µin/in-°F Flow, -40F to 200F; ASTM E 831
Thermal Conductivity0.19 W/m-K1.32 BTU-in/hr-ft²-°F ASTM C 177
Deflection Temperature at 0.46 MPa (66 psi)138 °C280 °F 0.250 inch, unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi)132 °C270 °F 0.250 inch, unannealed; ASTM D 648
Vicat Softening Point152 °C305 °F Rate B; ASTM D 1525
UL RTI, Electrical130 °C266 °F UL 746B
UL RTI, Mechanical with Impact120 °C248 °F UL 746B
UL RTI, Mechanical without Impact130 °C266 °F UL 746B
Flammability, UL94V-2V-2 0.058 in.
Flammability, UL94V-0V-0 0.118 in.

Optical Properties
Refractive Index1.5861.586 ASTM D 542
Haze1 %1 % 0.100 inch; ASTM D 1003
Transmission, Visible85 %85 % 0.100 inch; ASTM D 1003

Descriptive Properties
Radiant Panel ListingUL tested 
UL File Number, USAE121562 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.