MatWeb, The Online Materials Database
SABIC Innovative Plastics LEXAN FL900S Polycarbonate (Europe)
Subcategory: Polycarbonate; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their European product line.
Physical Properties | Original Value | Comments |
|
Density | 0.95 g/cc | ASTM D 792 |
Filler Content | 5 % | ASTM D 229 |
Water Absorption | 0.15 % | 24 hours; ASTM D 570 |
Water Absorption at Saturation | 0.35 % | 23C; ISO 62 |
Linear Mold Shrinkage | 0.005 - 0.007 cm/cm | Flow; ASTM D 955 |
Mechanical Properties |
|
Tensile Strength, Ultimate | 42 MPa | ASTM D 638 |
Elongation at Break | 5 % | ASTM D 638 |
Tensile Modulus | 2 GPa | DIN 53457 |
Flexural Modulus | 2.4 GPa | DIN 53457 |
Flexural Strength | 80 MPa | DIN 53452 |
Gardner Impact | 50 J | GE Test |
Electrical Properties |
|
Dielectric Constant | 2.3 | 1 MHz; IEC 60250 |
Dielectric Constant | 2.41 | 100 Hz; IEC 60250 |
Dissipation Factor | 0.0029 | 100 Hz; IEC 60250 |
Dissipation Factor | 0.01 | 1 MHz; IEC 60250 |
Thermal Properties |
|
CTE, linear 20°C | 35 µm/m-°C | 23C-80C, flow; ISO 11359-2 |
Specific Heat Capacity | 0.28 J/g-°C | ASTM C 351 |
Thermal Conductivity | 0.15 W/m-K | ISO 8302 |
Deflection Temperature at 0.46 MPa (66 psi) | 137 °C | ASTM D 648 |
Deflection Temperature at 1.8 MPa (264 psi) | 127 °C | ASTM D 648 |
UL RTI, Electrical | 80 °C | UL 746B |
UL RTI, Mechanical with Impact | 80 °C | UL 746B |
UL RTI, Mechanical without Impact | 80 °C | UL 746B |
Flammability, UL94 | V-0 | 6 mm |
Flammability, UL94 | 7 | 94-6 mm |
Oxygen Index | 35 % | ISO 4589 |
Descriptive Properties | |
%; Flexural Creep, 300 hours, 6.9 MPa | 0.4 | ASTM D 674 |
Ball Pressure Test, 125 C +/- 2 C | PASSES | IEC 60035-1 |
Ball Pressure Test, 75 C +/- 2 C | PASSES | IEC 60035-1 |
|
|
|
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
|