Physical PropertiesOriginal ValueComments
Density1.2 g/cc ISO 1183
Moisture Absorption at Equilibrium0.15 % (23 C / 50% RH) 1L; ISO 15512
Water Absorption at Saturation0.35 % 23C; ISO 62
Linear Mold Shrinkage0.005 - 0.007 cm/cm Flow; ASTM D 955
Melt Flow6 g/10 min cm3/10min; Melt Volume Rate, MVR at 300C/1.2 kg; ISO 1133

Mechanical Properties
Hardness, H358/3095 MPa ISO 2039/1
Tensile Strength, Ultimate60 MPa 50 mm/min; ISO 527
Tensile Strength, Yield63 MPa 50 mm/min; ISO 527
Elongation at Break100 % 50 mm/min; ISO 527
Elongation at Yield6 % 50 mm/min; ISO 527
Tensile Modulus2.3 GPa 1 mm/min; ISO 527
Flexural Modulus2.35 GPa 2 mm/min; ISO 178
Flexural Yield Strength90 MPa 2 mm/min; ISO 178
Izod Impact, Notched (ISO)11 kJ/m² 80*10*4 +23 C; ISO 180/ 1A
Izod Impact, Unnotched (ISO)NB 80*10*4 +23 C; ISO 180/ 1U
Izod Impact, Unnotched Low Temp (ISO)NB 80*10*4 -30 C; ISO 180/ 1U
Izod Impact, Notched, Low Temp (ISO)9 kJ/m² 80*10*4 -30 C; ISO 180/ 1A

Thermal Properties
CTE, linear 20°C70 µm/m-°C 23C-80C, flow; ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi)138 °C HDT/Be, 0.45MPa Edgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi)127 °C HDT/Ae, 1.82 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point144 °C B/50; ISO 306
Vicat Softening Point145 °C B/120; ISO 306

Descriptive Properties
Ball Pressure Test, 125 C +/- 2 CPASSES IEC 60035-1

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.