MatWeb, The Online Materials Database
SABIC Innovative Plastics LEXAN HP2 Polycarbonate (Europe)
Subcategory: Polycarbonate; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their European product line. This product is also a part of their North American product line.
Physical Properties | Original Value | Comments |
|
Density | 1.2 g/cc | ASTM D 792 |
Density | 1.2 g/cc | ISO 1183 |
Water Absorption | 0.1 % | 24 hours; ASTM D 570 |
Moisture Absorption at Equilibrium | 0.15 % | (23 C / 50% RH) 1L; ISO 15512 |
Water Absorption at Saturation | 0.35 % | 23C; ISO 62 |
Water Absorption at Saturation | 0.58 % | 100 C; ASTM D 570 |
Linear Mold Shrinkage | 0.005 - 0.007 cm/cm | Flow; ASTM D 955 |
Melt Flow | 21 g/10 min | cm3/10min; Melt Volume Rate, MVR at 300C/1.2 kg; ISO 1133 |
Mechanical Properties |
|
Hardness, Rockwell M | 70 | ISO 2039/2 |
Hardness, H358/30 | 95 MPa | ISO 2039/1 |
Tensile Strength, Ultimate | 65 MPa | 50 mm/min; ISO 527 |
Tensile Strength, Yield | 63 MPa | 50 mm/min; ISO 527 |
Elongation at Break | 100 % | 50 mm/min; ISO 527 |
Elongation at Yield | 6 % | 50 mm/min; ISO 527 |
Tensile Modulus | 2.35 GPa | 1 mm/min; ISO 527 |
Flexural Modulus | 2.3 GPa | 2 mm/min; ISO 178 |
Flexural Yield Strength | 90 MPa | 2 mm/min; ISO 178 |
Izod Impact, Notched | 6 J/cm | 23 C; ASTM D 256 |
Izod Impact, Notched (ISO) | 12 kJ/m² | 80*10*4 +23 C; ISO 180/ 1A |
Izod Impact, Unnotched (ISO) | NB | 80*10*4 +23 C; ISO 180/ 1U |
Izod Impact, Unnotched Low Temp (ISO) | NB | 80*10*4 -30 C; ISO 180/ 1U |
Izod Impact, Notched, Low Temp | 1.2 J/cm | at -40 C; ASTM D 256 |
Izod Impact, Notched, Low Temp (ISO) | 10 kJ/m² | 80*10*4 -30 C; ISO 180/ 1A |
Charpy Impact Unnotched | NB | 23C, Unnotch Edgew 80*10*4 sp=62; ISO 179/1eU |
Charpy Impact, Unnotched Low Temp | NB | at -30C, Unnotch Edgew 80*10*4 sp=62; ISO 179/1eU |
Charpy Impact, Notched | 3.5 J/cm² | 23 C; ISO 179/2C |
Taber Abrasion, mg/1000 Cycles | 10 | CS-17, 1 kg; GE Test |
Electrical Properties |
|
Volume Resistivity | Min 1e+015 ohm-cm | IEC 60093 |
Surface Resistivity per Square | Min 1e+015 ohm | ROA; IEC 60093 |
Dielectric Constant | 2.7 | 50 Hz; IEC 60250 |
Dielectric Constant | 2.7 | 1 MHz; IEC 60250 |
Dielectric Strength | 15 kV/mm | Short time, 3.2 mm; ASTM D 149 |
Dielectric Strength | 17 kV/mm | in oil, 3.2 mm; IEC 60243-1 |
Dissipation Factor | 0.001 | 50 Hz; IEC 60250 |
Dissipation Factor | 0.01 | 1 MHz; IEC 60250 |
Arc Resistance | 119 sec | Tungsten; ASTM D 495 |
Hot Wire Ignition, HWI | 48 sec | UL 746A |
High Voltage Arc-Tracking Rate, HVTR | 1.8 mm/min | UL 746A |
Thermal Properties |
|
CTE, linear 20°C | 70 µm/m-°C | 23C-80C, flow; ISO 11359-2 |
Thermal Conductivity | 0.2 W/m-K | ISO 8302 |
Hot Ball Pressure Test | Max 140 °C | IEC 60335-1 |
Deflection Temperature at 0.46 MPa (66 psi) | 133 °C | HDT/Be, 0.45MPa Edgew 120*10*4 sp=100mm; ISO 75/Be |
Deflection Temperature at 1.8 MPa (264 psi) | 122 °C | HDT/Ae, 1.82 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae |
Deflection Temperature at 1.8 MPa (264 psi) | 138 °C | ASTM D 648 |
Vicat Softening Point | 140 °C | B/50; ISO 306 |
Vicat Softening Point | 141 °C | B/120; ISO 306 |
Vicat Softening Point | 153 °C | Rate B; ASTM D 1525 |
Vicat Softening Point | 153 °C | VST/A/120; DIN 53460 |
Flammability, UL94 | HB | 3 mm; UL 94 by GE |
Flammability, UL94 | HB | 1.5 mm |
Flammability, UL94 | HB | 1.5 mm; UL 94 by GE |
Oxygen Index | 25 % | ISO 4589 |
Glow Wire Test | 850 °C | Passes at 1 mm; IEC 60695-2-1 |
Optical Properties |
|
Refractive Index | 1.586 | ISO 489 |
Haze | Max 0.8 % | ASTM D 1003 |
Transmission, Visible | 88 - 90 % | ASTM D 1003 |
Descriptive Properties | |
Ball Pressure Test, 125 C +/- 2 C | PASSES | IEC 60035-1 |
Hot Mandrel Test, 300 C | PASSES | CEE10/IIed |
Water Absorption, 24 hours, mg | 10 | DIN 53495 |
|
|
|
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
|