MatWeb, The Online Materials Database
SABIC Innovative Plastics LEXAN ML3286 Polycarbonate (Europe)
Subcategory: Polycarbonate; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their European product line.
Physical Properties | Metric | English | Comments |
|
Density | 1.33 g/cc | 0.048 lb/in³ | ISO 1183 |
Density | 1.33 g/cc | 0.048 lb/in³ | ASTM D 792 |
Moisture Absorption at Equilibrium | 0.12 % | 0.12 % | (23 C / 50% RH) 1L; ISO 15512 |
Water Absorption at Saturation | 0.3 % | 0.3 % | 23C; ISO 62 |
Linear Mold Shrinkage | 0.002 - 0.006 cm/cm | 0.002 - 0.006 in/in | Flow; ASTM D 955 |
Melt Flow | 5 g/10 min | 5 g/10 min | cm3/10min; Melt Volume Rate, MVR at 300C/1.2 kg; ISO 1133 |
Mechanical Properties |
|
Tensile Strength, Ultimate | 50 MPa | 7250 psi | 5 mm/min; ISO 527 |
Tensile Strength, Ultimate | 80 MPa | 11600 psi | ASTM D 638 |
Elongation at Break | 5 % | 5 % | 5 mm/min; ISO 527 |
Tensile Modulus | 4 GPa | 580 ksi | 1 mm/min; ISO 527 |
Flexural Modulus | 4.5 GPa | 653 ksi | 2 mm/min; ISO 178 |
Flexural Modulus | 5 GPa | 725 ksi | DIN 53457 |
Flexural Strength | 95 MPa | 13800 psi | 2 mm/min; ISO 178 |
Izod Impact, Notched | 0.6 J/cm | 1.12 ft-lb/in | 23 C; ASTM D 256 |
Izod Impact, Notched (ISO) | NB | NB | 80*10*4 +23 C; ISO 180/ 1A |
Izod Impact, Notched, Low Temp (ISO) | 20 kJ/m² | 9.52 ft-lb/in² | 80*10*4 -30 C; ISO 180/ 1A |
Charpy Impact, Notched | NB | NB | 23C, V-notch Edgew 80*10*4 sp=62; ISO 179/1eA |
Electrical Properties |
|
Volume Resistivity | Min 1e+015 ohm-cm | Min 1e+015 ohm-cm | IEC 60093 |
Surface Resistivity per Square | Min 1e+015 ohm | Min 1e+015 ohm | ROA; IEC 60093 |
Dielectric Constant | 2.9 | 2.9 | 1 MHz; IEC 60250 |
Dielectric Constant | 3 | 3 | 50 Hz; IEC 60250 |
Dielectric Strength | 16 kV/mm | 406 kV/in | in oil, 3.2 mm; IEC 60243-1 |
Dissipation Factor | 0.001 | 0.001 | 50 Hz; IEC 60250 |
Dissipation Factor | 0.01 | 0.01 | 1 MHz; IEC 60250 |
Thermal Properties |
|
CTE, linear 20°C | 30 µm/m-°C | 16.7 µin/in-°F | 23C-80C, flow; ISO 11359-2 |
Thermal Conductivity | 0.22 W/m-K | 1.53 BTU-in/hr-ft²-°F | ISO 8302 |
Deflection Temperature at 1.8 MPa (264 psi) | 125 °C | 257 °F | HDT/Ae, 1.82 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae |
Flammability, UL94 | HB | HB | 1.6 mm |
Flammability, UL94 | HB | HB | 1.6 mm; UL 94 by GE |
Glow Wire Test | 850 °C | 1560 °F | Passes at 1 mm; IEC 60695-2-1 |
Descriptive Properties | |
Ball Pressure Test, 125 C +/- 2 C | PASSES | IEC 60035-1 |
|
|
|
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
|