Physical PropertiesOriginal ValueComments
Density1.2 g/cc ASTM D 792
Density1.2 g/cc ISO 1183
Moisture Absorption at Equilibrium0.15 % (23 C / 50% RH) 1L; ISO 15512
Water Absorption at Saturation0.35 % 23C; ISO 62
Linear Mold Shrinkage0.005 - 0.007 cm/cm Flow; ASTM D 955
Melt Flow5 g/10 min cm3/10min; Melt Volume Rate, MVR at 300C/1.2 kg; ISO 1133

Mechanical Properties
Hardness, H358/3095 MPa ISO 2039/1
Tensile Strength, Ultimate65 MPa 50 mm/min; ISO 527
Tensile Strength, Yield60 MPa 50 mm/min; ISO 527
Elongation at Break120 % 50 mm/min; ISO 527
Elongation at Yield7 % 50 mm/min; ISO 527
Tensile Modulus2.35 GPa 1 mm/min; ISO 527
Flexural Modulus2.3 GPa 2 mm/min; ISO 178
Flexural Yield Strength85 MPa 2 mm/min; ISO 178
Izod Impact, Notched (ISO)65 kJ/m² 80*10*4 +23 C; ISO 180/ 1A
Izod Impact, Unnotched (ISO)NB 80*10*4 +23 C; ISO 180/ 1U
Izod Impact, Unnotched Low Temp (ISO)NB 80*10*4 -30 C; ISO 180/ 1U
Izod Impact, Notched, Low Temp (ISO)13 kJ/m² 80*10*4 -30 C; ISO 180/ 1A
Charpy Impact, Notched, Low Temp1.2 J/cm² at -30C, V-notch Edgew 80*10*4 sp=62; ISO 179/1eA
Charpy Impact, Notched6 J/cm² 23C, V-notch Edgew 80*10*4 sp=62; ISO 179/1eA
Taber Abrasion, mg/1000 Cycles10 CS-17, 1 kg; GE Test

Electrical Properties
Volume ResistivityMin 1e+015 ohm-cm IEC 60093
Surface Resistivity per SquareMin 1e+015 ohm ROA; IEC 60093
Dielectric Constant2.7 50 Hz; IEC 60250
Dielectric Constant2.7 1 MHz; IEC 60250
Dielectric Strength16.5 kV/mm Short time, 1.0 mm; IEC 60243-1
Dielectric Strength17 kV/mm in oil, 3.2 mm; IEC 60243-1
Dissipation Factor0.001 50 Hz; IEC 60250
Dissipation Factor0.01 1 MHz; IEC 60250

Thermal Properties
CTE, linear 20°C70 µm/m-°C 23C-80C, flow; ISO 11359-2
Thermal Conductivity0.2 W/m-K ISO 8302
Deflection Temperature at 0.46 MPa (66 psi)142 °C HDT/Be, 0.45MPa Edgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi)127 °C HDT/Ae, 1.82 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point146 °C B/50; ISO 306
Vicat Softening Point148 °C B/120; ISO 306
Glow Wire Test850 °C Passes at 1 mm; IEC 60695-2-1

Optical Properties
Refractive Index1.586 ISO 489
HazeMax 0.8 % ASTM D 1003
Transmission, Visible88 - 90 % ASTM D 1003

Descriptive Properties
Ball Pressure Test, 125 C +/- 2 CPASSES IEC 60035-1

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.