MatWeb, The Online Materials Database
SABIC Innovative Plastics LEXAN® SP1310R Polycarbonate, Unfilled, Injection Grade
Subcategory: Polycarbonate; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Data for 3.2 mm (1/8 in) samples unless otherwise noted. Data provided by GE Plastics.
Physical Properties | Original Value | Comments |
|
Density | 1.18 g/cc | ASTM D792 |
Water Absorption | 0.13 % | 24 hrs; 20°C; ASTM D570 |
Linear Mold Shrinkage | 0.005 - 0.007 cm/cm | 3.2 mm sample |
Melt Flow | 10 g/10 min | 300°C/1.2kg; ASTM D1238 |
Mechanical Properties |
|
Tensile Strength, Ultimate | 62 MPa | ASTM D638 |
Elongation at Break | 110 % | ASTM D638 |
Modulus of Elasticity | 2.1 GPa | ASTM D638 |
Flexural Modulus | 2.4 GPa | 3.2 mm sample; ASTM D790 |
Flexural Yield Strength | 96 MPa | ASTM D790 |
Izod Impact, Notched | 9.1 J/cm | 3.2 mm sample; ASTM D256 |
Thermal Properties |
|
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C | 6.4 mm sample; ASTM D648 |
Deflection Temperature at 1.8 MPa (264 psi) | 111 °C | 6.4 mm (0.25 in.) sample; ASTM D648 |
Vicat Softening Point | 132 °C | 5 kg; ASTM D1525 |
UL RTI, Electrical | 75 °C | UL 746B |
UL RTI, Mechanical with Impact | 75 °C | UL 746B |
UL RTI, Mechanical without Impact | 75 °C | UL 746B |
Flammability, UL94 | HB | 1.1 mm |
Processing Properties |
|
Processing Temperature | 293 - 315 °C | Suggested injection molding melt temperature |
Mold Temperature | 71 - 93 °C | |
Drying Temperature | 121 °C | |
Dry Time | 3 - 4 hour | 48 hr Max |
|
|
|
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
|