MatWeb, The Online Materials Database
SABIC Innovative Plastics LexanŽ 9034 Polycarbonate Sheet
Subcategory: Polycarbonate; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: LexanŽ 9034 uncoated polycarbonate sheet is the standard grade of LEXAN sheet for transparent protective glazing. High-impact LEXAN 9034 sheet can be utilized for primary glazing, or on either side of existing glazing for economical protection against breakage or intrusion. A better insulator than glass, LEXAN 9034 sheet contributes to lower energy costs. Information provided by Aurora Technologies.
Physical Properties | Metric | English | Comments |
|
Water Absorption | 0.15 % | 0.15 % | |
Mechanical Properties |
|
Hardness, Rockwell M | 70 | 70 | |
Tensile Strength, Yield | 62.1 MPa | 9000 psi | |
Flexural Strength | 93.1 MPa | 13500 psi | |
Compressive Strength | 86.2 MPa | 12500 psi | |
Shear Strength | 41.4 MPa | 6000 psi | |
Izod Impact, Notched | 6.41 - 8.54 J/cm | 12 - 16 ft-lb/in | Edgewise |
Electrical Properties |
|
Dielectric Constant | 2.96 | 2.96 | 10 Hz |
Dielectric Constant | 3.17 | 3.17 | 60 Hz |
Dissipation Factor | 0.0009 | 0.0009 | 60 Hz |
Dissipation Factor | 0.01 | 0.01 | 1 MHz |
Arc Resistance | 10 - 11 sec | 10 - 11 sec | Stainless Steel Strips |
Arc Resistance | 120 sec | 120 sec | Tungsten Electrodes |
Thermal Properties |
|
Flammability Test | Min 1 | Min 1 | inches; Horizontal Burn (Flame Spread) |
Optical Properties |
|
Transmission, Visible | 88 % | 88 % | 1/8 in disk |
Descriptive Properties | |
Color | Clear | |
|
|
|
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
|