MatWeb, The Online Materials Database
SABIC Innovative Plastics Lexan® 9600 Polycarbonate Sheet
Subcategory: Polycarbonate; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Lexan® 9600 sheet offers improved flammability characteristics than conventional LEXAN polycarbonate sheet. It is formulated to meet the standards of UL Bulletin, Class I. Developed to meet industry flammability codes, LEXAN 9600 sheet is widely used in power tools, electrical appliances, safety equipment and aircraft components. The improved flammability and slightly higher heat deflection temperature of LEXAN 9600 sheet are accompanied by essentially the same physical, electrical, chemical and fabricating properties exhibited by standard LEXAN Sheet. Information provided by Aurora Technologies.
Physical Properties | Metric | English | Comments |
|
Water Absorption | 0.2 % | 0.2 % | |
Mechanical Properties |
|
Tensile Strength, Ultimate | 62.1 MPa | 9000 psi | |
Tensile Strength, Yield | 65.5 MPa | 9500 psi | |
Elongation at Break | 95 % | 95 % | |
Flexural Modulus | 2.55 GPa | 370 ksi | |
Flexural Strength | 93.1 MPa | 13500 psi | |
Compressive Strength | 86.2 MPa | 12500 psi | |
Izod Impact, Unnotched | NB | NB | |
Izod Impact, Notched | 6.41 - 8.54 J/cm | 12 - 16 ft-lb/in | Edgewise |
Izod Impact, Notched | 1.28 J/cm | 2.4 ft-lb/in | |
Thermal Properties |
|
CTE, linear 68°F | 67.5 µm/m-°C | 37.5 µin/in-°F | |
Maximum Service Temperature, Air | 138 °C | 280 °F | Deflection Temp; Load not specified |
Flammability, UL94 | V-0 | V-0 | |
Optical Properties |
|
Transmission, Visible | 85 % | 85 % | 1/8 in disk |
Descriptive Properties | |
Color | Clear | |
|
|
|
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
|