ITW Devcon Rubber Repair / Castable Urethane Flexane® 80 Putty, Black


Subcategory: Adhesives, Sealants, and Coatings; Polymer; Polyurethane, TS; Thermoset

Material Notes:

Information provided by ITW Devcon

Physical PropertiesOriginal ValueComments
Density0.0426 lb/in³ 

Mechanical Properties
Hardness, Shore A87 Cured; ASTM D2240
Tensile Strength @ Break1700 psi ASTM D412
Elongation at BreakMax 300 % ASTM D412
Tear Strength300 pli ASTM D624
Taber Abrasion, mg/1000 Cycles280 H-18 wheel (1000 gram load)

Electrical Properties
Dielectric Strength350 V/mil ASTM D149

Thermal Properties
Maximum Service Temperature, Air120 °F wet
Maximum Service Temperature, Air180 °F dry
Shrinkage0.14 % Cured; ASTM D2566

Processing Properties
Cure Time12 hour Functional cure
Pot Life20 min at 75°F

Descriptive Properties
Coverage per pound, in² @ 1/4" thickness94 
Mix ratio by weight (Resin:Hardener)72:28 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.