ITW Devcon Rubber Repair / Castable Urethane Flexane® High Performance Putty, Black


Subcategory: Adhesives, Sealants, and Coatings; Polymer; Polyurethane, TS; Thermoset

Material Notes:

Information provided by ITW Devcon

Physical PropertiesMetricEnglishComments
Density1.18 g/cc0.0426 lb/in³ 

Mechanical Properties
Hardness, Shore A7878 Cured; ASTM D2240
Tensile Strength @ Break31 MPa4500 psi ASTM D412
Elongation at BreakMax 600 %Max 600 % ASTM D412
Tear Strength70.1 kN/m400 pli ASTM D624
Taber Abrasion, mg/1000 Cycles140140 H-18 wheel (1000 gram load)

Electrical Properties
Dielectric Strength13.8 kV/mm350 V/mil ASTM D149

Thermal Properties
Maximum Service Temperature, Air48.9 °C120 °F wet
Maximum Service Temperature, Air82.2 °C180 °F dry
Shrinkage12 %12 % Cured (shrinkage due to solvent loss); ASTM D2566

Processing Properties
Cure Time960 min16 hour Functional cure
Pot Life10 min10 min at 75°F

Descriptive Properties
Coverage per pound, in² @ 1/4" thickness94 
Mix ratio by weight (Resin:Hardener)94:6 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.