MatWeb, The Online Materials Database
ITW Devcon Rubber Repair / Castable Urethane Flexane® 80 Liquid, Black
Subcategory: Adhesives, Sealants, and Coatings; Polymer; Polyurethane, TS; Thermoset
Material Notes:
Information provided by ITW Devcon
Physical Properties | Metric | English | Comments |
|
Density | 1.04 g/cc | 0.0377 lb/in³ | |
Viscosity | 10000 cP | 10000 cP | Mixed Viscosity |
Mechanical Properties |
|
Hardness, Shore A | 87 | 87 | Cured; ASTM D2240 |
Tensile Strength @ Break | 14.5 MPa | 2100 psi | ASTM D412 |
Elongation at Break | Max 650 % | Max 650 % | ASTM D412 |
Tear Strength | 61.4 kN/m | 350 pli | ASTM D624 |
Taber Abrasion, mg/1000 Cycles | 285 | 285 | H-18 wheel (1000 gram load) |
Electrical Properties |
|
Dielectric Strength | 13.8 kV/mm | 350 V/mil | ASTM D149 |
Thermal Properties |
|
Maximum Service Temperature, Air | 48.9 °C | 120 °F | wet |
Maximum Service Temperature, Air | 82.2 °C | 180 °F | dry |
Shrinkage | 0.18 % | 0.18 % | Cured; ASTM D2566 |
Processing Properties |
|
Cure Time | 960 min | 16 hour | Functional cure |
Pot Life | 30 min | 30 min | at 75°F |
Descriptive Properties | |
Coverage per pound, in² @ 1/4" thickness | 106 | |
Demolding Time, hours | 10 | |
Mix ratio by weight (Resin:Hardener) | 77:23 | |
|
|
|
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
|