LNP (SABIC Innovative Plastics) LEXAN® BFL2015 Polycarbonate


Subcategory: Polycarbonate; Polymer; Thermoplastic

Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.

Material Notes:

  • Forms: Pellets

Information provided by LNP, a GE Plastics Company.

Physical PropertiesOriginal ValueComments
Specific Gravity1.3 g/cc ASTM D792
Water Absorption0.14 % at 24 hrs; ASTM D570
Linear Mold Shrinkage0.0025 - 0.0035 cm/cm 3.20 mm; ASTM D955

Mechanical Properties
Tensile Strength, Yield84.3 MPa ASTM D638
Elongation at Break4 - 6 % ASTM D638
Flexural Modulus4.47 GPa ASTM D790
Flexural Strength133 MPa ASTM D790
Izod Impact, Notched0.91 J/cm ASTM D256

Thermal Properties
CTE, linear 20°C40 - 50 µm/m-°C TMA, -30°C to 30°C
Deflection Temperature at 0.46 MPa (66 psi)142 °C Unannealed (3.20 mm); ASTM D648
Flammability, UL94V-0 1.50mm

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.