MatWeb, The Online Materials Database
LNP (SABIC Innovative Plastics) LEXAN® EXCP0001 Polycarbonate, 16% Carbon Powder
Subcategory: Filled/Reinforced Thermoplastic; Polycarbonate; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Electronic packaging applications. - Features: Electrically Conductive, Low to none Ion content
- Forms: Pellets
- Processing Method: Injection Molding
Information provided by LNP, a GE Plastics Company.
Physical Properties | Original Value | Comments |
|
Specific Gravity | 1.27 g/cc | ASTM D792 |
Linear Mold Shrinkage | 0.006 - 0.008 cm/cm | 3.18 mm; ASTM D955 |
Linear Mold Shrinkage, Transverse | 0.006 - 0.008 cm/cm | 3.18 mm; ASTM D955 |
Melt Flow | 27 g/10 min | 300°C / 5.0 kg; ASTM D1238 |
Mechanical Properties |
|
Tensile Strength at Break | 59.3 MPa | Type I, 5mm/min; ASTM D638 |
Tensile Strength, Yield | 63.4 MPa | Type I, 5mm/min; ASTM D638 |
Elongation at Break | 13 % | Type I, 5mm/min; ASTM D638 |
Elongation at Yield | 13 % | Type I, 5mm/min; ASTM D638 |
Flexural Modulus | 2.9 GPa | (50.8 mm Span) 1mm/min; ASTM D790 |
Flexural Strength | 105 MPa | at Break, (50.8 mm Span) 1mm/min; ASTM D790 |
Izod Impact, Notched | 0.48 J/cm | ASTM D256 |
Izod Impact, Unnotched | 16 J/cm | ASTM D256 |
Falling Dart Impact | 26.6 J | ASTM D3763 |
Electrical Properties |
|
Volume Resistivity | 300000 ohm-cm | ASTM D257 |
Surface Resistance | 100000 ohm | ASTM D257 |
Static Decay | Max 0.01 sec | 5000V to <50V; FTMS101B |
Thermal Properties |
|
Deflection Temperature at 0.46 MPa (66 psi) | 141 °C | Unannealed (3.18 mm); ASTM D648 |
Deflection Temperature at 1.8 MPa (264 psi) | 129 °C | Unannealed (3.18 mm); ASTM D648 |
Processing Properties |
|
Rear Barrel Temperature | 266 - 288 °C | |
Middle Barrel Temperature | 277 - 299 °C | |
Front Barrel Temperature | 288 - 310 °C | |
Nozzle Temperature | 282 - 304 °C | |
Melt Temperature | 288 - 310 °C | |
Mold Temperature | 71.1 - 93.3 °C | |
Drying Temperature | 121 °C | |
Dry Time | 3 - 8 hour | |
Moisture Content | 0.02 % | Suggested |
Back Pressure | 0.345 - 0.689 MPa | |
Clamp Pressure | 41 - 69 MPa | |
Shot Size | 40 - 60 % | Suggested |
Vent Depth | 0.0025 - 0.0076 cm | |
Screw Speed | 40 - 70 rpm | |
|
|
|
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
|