MatWeb, The Online Materials Database
LNP (SABIC Innovative Plastics) LEXAN® EXCP0088 Polycarbonate, 20% Glass Fiber Reinforcement
Subcategory: Filled/Reinforced Thermoplastic; Polycarbonate; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Business equipment applications. Will be commercialized as LG2000HT. UL94 HB rating pending. - Features: General Purpose
- Forms: Pellets
- Processing Method: Injection Molding
Information provided by LNP, a GE Plastics Company.
Physical Properties | Metric | English | Comments |
|
Specific Gravity | 1.34 g/cc | 0.0484 lb/in³ | ASTM D792 |
Mechanical Properties |
|
Tensile Strength at Break | 96.5 MPa | 14000 psi | Type I, 5mm/min; ASTM D638 |
Tensile Strength, Yield | 96.5 MPa | 14000 psi | Type I, 5mm/min; ASTM D638 |
Elongation at Break | 2.9 % | 2.9 % | Type I, 5mm/min; ASTM D638 |
Elongation at Yield | 2.9 % | 2.9 % | Type I, 5mm/min; ASTM D638 |
Tensile Modulus | 6.24 GPa | 905 ksi | 5 mm/min; ASTM D638 |
Flexural Modulus | 6.24 GPa | 905 ksi | (50.8 mm Span) 1mm/min; ASTM D790 |
Flexural Strength | 159 MPa | 23100 psi | at Break, (50.8 mm Span) 1mm/min; ASTM D790 |
Izod Impact, Notched | 0.801 J/cm | 1.5 ft-lb/in | ASTM D256 |
Izod Impact, Unnotched | 6.57 J/cm | 12.3 ft-lb/in | ASTM D256 |
Thermal Properties |
|
Deflection Temperature at 0.46 MPa (66 psi) | 142 °C | 288 °F | Unannealed (3.18 mm); ASTM D648 |
Deflection Temperature at 1.8 MPa (264 psi) | 138 °C | 280 °F | Unannealed (3.18 mm); ASTM D648 |
Processing Properties |
|
Rear Barrel Temperature | 271 - 293 °C | 520 - 559 °F | |
Middle Barrel Temperature | 282 - 304 °C | 540 - 579 °F | |
Front Barrel Temperature | 293 - 316 °C | 559 - 601 °F | |
Nozzle Temperature | 288 - 310 °C | 550 - 590 °F | |
Melt Temperature | 293 - 316 °C | 559 - 601 °F | |
Mold Temperature | 71.1 - 93.3 °C | 160 - 200 °F | |
Drying Temperature | 121 °C | 250 °F | |
Dry Time | 3 - 48 hour | 3 - 48 hour | |
Moisture Content | 0.02 % | 0.02 % | Suggested |
Back Pressure | 0.345 - 0.689 MPa | 50 - 99.9 psi | |
Clamp Pressure | 41 - 69 MPa | 5950 - 10000 psi | |
Shot Size | 40 - 60 % | 40 - 60 % | Suggested |
Vent Depth | 0.0025 - 0.0076 cm | 0.000984 - 0.00299 in | |
Screw Speed | 40 - 70 rpm | 40 - 70 rpm | |
|
|
|
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
|