GE Advanced Ceramics NX10 Boron Nitride (BN) Powder

 

Subcategory: Nitride; Additive/Filler for Polymer

Material Notes:
GE Advanced Ceramics has recently launched an innovative new NX line of boron nitride (BN) powders - grades NX1, NX5, NX9, and NX10. This line of products offers an economical way to achieve many of the benefits of BN in a wide range of applications. The NX line makes BN accessible to users of alternate materials, such as aluminum nitride, alumina, and fused silica, who may have previously ruled out BN.

NX grades are all fine hexagonal crystalline powders (95%-100% -325 mesh), and are available in a range of purities and surface areas to suit your specific applications.

NX10 has a mean particle size of approximately 10 microns and is a higher purity grade than NX9.

Applications: GE Advanced Ceramics NX grades are candidates for use in a wide range of demanding applications for which BN is generally considered, including:

  • Lubricants and release agents for high-temperature metal & glass processing
  • Refractory coatings
  • Base material for hot pressed solids and metal-matrix or ceramic-metal composites
  • Processing and final-product enhancement of plastics, including nucleation of solid and foamed products.
  • Thermal management materials (adhesives, gap-fillers, encapsulants, polymer matrices, etc.) for electronics applications

Information provided by GE Advanced Ceramics.

Available Properties
  • Density
  • Particle Size
  • Specific Surface Area
  • Calcium
  • Carbon
  • Color
  • Crystal Type
  • Oxygen
  • Sol. Borate
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。