Piezo Kinetics, Inc. 100 Lead Metaniobate Piezoelectric

 

Subcategory: Oxide, Other; Piezoelectric; Oxide

Key Words: PKI 100, Lead Niobium Oxides

Material Notes:
Lead Metaniobate exhibits properties not usually present in other types of piezoelectric ceramics. The noteworthy facts are its low mechanical QM, negligible aging, wide range of operating temperatures and small values for lateral and planar coupling compared to longitudinal coupling. The low QM enhances the use of PKI 100 material in the construction of wide bandwidth sensors for high frequency pulse echo measurements that require a short pulse and critical resolution. Its negligible aging helps simplify circuit design. Wide variations in temperature have limited effect on its dielectric and piezoelectric properties making it ideal for high temperature applications. Its high longitudinal coupling compared to lateral and planar coupling allows it to generate a better response under hydrostatic pressures and makes it useful for underwater sonar equipment.

Property data at 25°C. Information supplied by Piezo Kinetics, Inc.

Available Properties
  • Density
  • Curie Temperature
  • Dielectric Constant
  • Dissipation Factor
  • Piezoelectric Longitudinal Coupling Factor, k33
  • Piezoelectric Longitudinal Voltage Coefficient, g33, 10^-3 V-m/N
  • Piezoelectric Planar Coupling Factor, kp
  • Piezoelectric Mechanical Q
  • Piezoelectric Longitudinal Charge Coefficient, d33, 10^-12 m/V
  • Maximum Service Temperature, Air
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。