Pyrotek Dense Fused Silica Pre-Cast Shapes

 

Subcategory: Oxide, Silicon; Oxide

Material Notes:
Pyrocast Dense Fused Silica is an economical product for shapes demanding thermal shock resistance at temperatures. Pyrocast DFS stands up to repeated use in molten metal casting in aluminum, copper, zinc, brass, steel, glass, and aerospace applications. It is durable and resists breakage during handling and cleaning. Components made from Pyrocast Dense Fused Silica resist cracking due to the material's low thermal expansion.

Applications

  • Spouts
  • Control pins
  • Mounting seats (inserts)
  • Pre-cast trough tiles
  • Thimbles
  • Wear plates
  • Trough dams

Advantages

  • Resistant to thermal shock
  • Superior strength
  • Low thermal expansion
  • Economically priced
  • Resistant to surface corrosion
  • Able to rapidly cycle
  • Computer controlled firing
  • Superior material consistency

Information provided by Pyrotek.

Available Properties
  • Density
  • Open Porosity
  • Modulus of Rupture
  • Compressive Strength
  • CTE, linear 20°C
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。