Pyrotek MT-29B Microporous Insulating Board

 

Material Notes:
MT-29B has the low thermal conductivity. Its cellular structure contributes to its low-weight, good compressive strength, and low shrinkage at high temperatures.

Applications
Backup insulation for:

  • Troughs
  • Filter bowls
  • Furnace linings
  • Transfer crucibles
  • Door insulation

Advantages

  • Low thermal conductivity
  • Reduces warping of vessels and troughing
  • Promotes greater temperature control
  • Minimizes heat transfer
  • Can be designed to be reused
  • Minimizes hot face temperature of vessels
  • Provides low shrinkage at high temperatures
  • Not wet by molten aluminum

Information provided by Pyrotek.

Available Properties
  • Density
  • Compressive Strength
  • Thermal Conductivity at Elevated Temperature
  • Maximum Service Temperature, Air
  • Shrinkage
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。