Reade Advanced Materials Bentonite Powder (BaTiSi3O9)

 

Subcategory: Clay

Key Words: BaTiSi3O9, Bentonite, taylorite, fuller's earth, Wyoming sodium bentonite, sodium montmorillonite, saponite, hectorite, hormite clay

Material Notes:
Description: A rock composed essentially of a crystalline clay-like mineral formed by devitrification and the accompanying chemical alteration of a glassy igneous material, usually a tuff or volcanic ash.
Uses: Used as a foundry sand, paints, fuller's earth, drilling mud, bleaching clay, filtering agents, water impedance, inks, additive to ceramic materials, and iron ore pelletizing. Used in pharmaceuticals, beverage, food, cosmetics, and personal care products (Suspending agent, gellant and binder). Bentonite possesses thixotropic properties and deposits a thin water proofing film on the walls of the bore holes & thus renders permeable formations impermeable. Both natural & synthetic Bentonite are used in preparation of drilling muds. It is mainly used as circulation mud in rotary system of drilling for oil. The main purpose of Bentonite is to lubricate & cool the rotary cutting bits, carry away rock cutting fragments & to act as a seal against the escape of gas from the bore hole & to improve & prevent the hole from blowing out. Another function of such Bentonite based fluids is to condition the wall of the drill hole to prevent caving.
Physical Properties Available: Numerous particle size options are available in the lower micron area from a mean particle size of 2.5 to 4.0 microns.

Information provided by Reade Advanced Materials.

Available Properties
  • Density
  • Specific Gravity
  • pH
  • Specific Surface Area
  • Color
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。