Reade Advanced Materials Diatomite Powder

 

Material Notes:
Description: Diatomite is a sedimentary rock, white to light yellow in color, composed of the fossilized skeletons of diatoms, one celled algae-like plants which accumulated in marine or lacustrine environments. The honeycomb silica structures gives diatomite useful characteristics such as high absorptive capacity and surface area, chemical stability, and low bulk density.

Diatomite is principally used in filtration of various alcoholic beverages, sugar, oil, organic and inorganic chemicals, and water. It is also used as a filler in absorbents for pet litter and oil spills. Other uses are: pesticide carrier, roughness and flatting agent in paint; an anti-blocking agent in polyethylene film; a soft abrasive in silver and automotive polishes; or as bulk extender. Small amounts of diatomite are used as a thermal insulator and catalyst carrier.
Physical Properties Available: Fine grained powder

Information provided by Reade Advanced Materials.

Available Properties
  • Specific Gravity
  • pH
  • Refractive Index
  • Color
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。