Schott Dark ROBAX® Glass Ceramic

 

Subcategory: Glass; Glass Ceramic; Optical

Material Notes:
Dark ROBAX® is an infra-red transparent glass-ceramic having virtually zero thermal expansion and sufficient mechanical resistance required for all standard applications. It is produced in rolled sheets with one surface flat and one surface textured with nubs. As a result of its extremely low thermal expansion, Dark ROBAX® can be subjected to extreme temperature differences. Even when used in high temperature conditions, Dark ROBAX® maintains excellent stability of form. Dark ROBAX® can be further processed mechanically using all of the normal methods of glass processing.

Applications: Dark ROBAX® possesses a high degree of resistance against thermal stresses and chemical surface attacks. Its diverse range of applications include: high temperature vision windows for UV and visual light blocking, heat insulators, commercial heating equipment, and electronics.

Information provided by SCHOTT North America.

Available Properties
  • Density
  • Modulus of Elasticity
  • Flexural Strength
  • Poissons Ratio
  • Shear Modulus
  • Volume Resistivity
  • Dielectric Constant
  • Dissipation Factor
  • CTE, linear 20°C
  • Specific Heat Capacity
  • Thermal Conductivity at Elevated Temperature
  • Maximum Service Temperature, Air
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。