Schott ROBAX® Glass Ceramic

 

Subcategory: Glass; Glass Ceramic; Optical

Material Notes:
ROBAX® is a highly transparent glass-ceramic having virtually zero thermal expansion and sufficient mechanical resistance required for all standard applications. It is produced in flat, rolled sheets.

As a result of its extremely low thermal expansion, ROBAX® can be subjected to extreme temperature differences. Even when used in high temperature conditions, ROBAX® maintains excellent stability of form. ROBAX® can be further processed mechanically using all of the normal methods of glass processing.

Applications: ROBAX® possesses a high degree of resistance against thermal stresses and chemical surface attacks. Its diverse range of applications include: chemical process sight glass, high temperature vision windows, heat insulators, commercial ovens/broilers, architectural and outdoor lighting, electronics and UV light wave blocking applications.

Information provided by SCHOTT North America.

Available Properties
  • Density
  • Modulus of Elasticity
  • Poissons Ratio
  • Shear Modulus
  • Volume Resistivity
  • Dielectric Constant
  • Dissipation Factor
  • CTE, linear 20°C
  • Specific Heat Capacity
  • Thermal Conductivity at Elevated Temperature
  • Maximum Service Temperature, Air
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。