Thermal Ceramics LA Bulk Saffil

 

Material Notes:
Saffil alumina fibers are high purity polycrystalline fibers designed for use in applications up to 2900°F (1600°C). Since their development in the early 1970’s Saffil fibers have been used successfully to overcome problems in demanding high temperature insulation and many other specialty applications.

Saffil fibers are produced by a unique solution extrusion process which ensures the highest levels of chemical purity and the lowest possible levels of shot content (non-fibrous particles).

The fiber is processed to ensure that a high level of alumina is converted into the extremely thermally stable alpha alumina phase. This process gives the finished product exceptional resistance to shrinkage and chemical attack at high temperature, while maintaining excellent flexibility and resilience characteristics.

Features:

  • Refractoriness - Low shrinkage at high temperature 2900°F (1600°C) ensures long life in the most demanding applications
  • Thermal Conductivity - Very low shot levels translate into low thermal conductivity, offering savings on fuel and rapid payback on investment
  • Resistance to Chemical Attack - High levels of alumina, low silica and trace element levels ensure chemical stability in the majority of industrial process conditions
  • Resilience - Unique method of manufacture and high classification temperature result in a fibre with exceptional resilience at high temperatures
  • Information provided by Thermal Ceramics

    Available Properties
    • Density
    • Loss On Ignition
    • Melting Point
    • Maximum Service Temperature, Air
    • Shrinkage
    • Fiber Diameter, Micron
    • Shot content
    • Solubility in Watier
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。