Thermal Ceramics PM Kaowool Low Temperature Boards

 

Subcategory: Kaolin

Material Notes:
Kaowool PM is manufactured to close tolerances with an excellent surface finish. Kaowool PM has a good thermal conductivity and can easily be die-cut.

Features:

  • Excellent thermal conductivity
  • Capability to withstand chemical attack
  • Board capabilities are 48 x 36 x 1/4 to 3" (120 x 90 x 0.625 to 7.5 cm) with the exception of PM Board which can be made 1/8" (3.125 cm) thick
  • Applications:

  • Appliance and heat processing insulation
  • Back up in steel ladle and torpedo cars
  • Backup insulation to dense refractories
  • Combustion chamber construction
  • Expansion joint material
  • Flue and chimney linings
  • Furnace, kiln, and oven hot face linings
  • General molten metal contact
  • Glass coffin walls
  • Glass regenerator insulation
  • Glass tank side, end wall and port neck
  • Glass tank wall and port neck insulation
  • Heat shields
  • High temperature gaskets and seals
  • High mechanical stress areas
  • Kiln furniture
  • Trough linings in contact with aluminum

    Information provided by Thermal Ceramics

    Available Properties
    • Density
    • Loss On Ignition
    • Modulus of Rupture
    • Compressive Strength
    • Thermal Conductivity
    • Melting Point
    • Maximum Service Temperature, Air
    • Shrinkage
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
  • 请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。