AMPCO METAL AMPCO® 15 Aluminum Bronze, Extruded Rod, ≤ 12.7 mm.

 

Subcategory: Copper Alloy; Nonferrous Metal; Bronze

Key Words: ASTM B-150 C61900; ASTM B-150 C62300; ASME SB-150 C62300; SAE J-463 C62300; AMS 4635

Material Notes:
A wrought aluminum-iron-copper alloy recommended for medium-duty applications involving wear and fatigue, especially where higher ductility is required for cold working. Ampco 15 alloy will maintain mechanical properties at temperatures up to 315°C. It has a machinability rating of 50%. The alloy provides excellent corrosion resistance to sea water and nonoxidizing mineral acids. Can be welded with gasshielded and shielded metal-arc processes. Brazing, soldering and oxyfuel gas welding are not recommended. Hot and cold formability is good with a forgeability rating of 75%. Ampco 15 alloy can be hot worked at temperatures from 760° to 900°C and annealed between 595° and 650°C. The consistent superiority of Ampco 15 alloy over commercial bronze is due, in large part, to the unique distribution of alloy microstructure, often referred to as the "Ampco-Phase". Only Ampco alloys offer this metallurgical advantage.

Applications: Uses include: cams; bushings; bearing retainer cages; valve stems and guides; sleeve bearings.

Available Properties
  • Density
  • Specific Gravity
  • Hardness, Brinell
  • Hardness, Rockwell B
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • Modulus of Rigidity
  • Compressive Yield Strength
  • Compressive Strength
  • Poissons Ratio
  • Charpy Impact
  • Izod Impact
  • Fatigue Strength
  • Electrical Resistivity
  • Magnetic Permeability
  • CTE, linear 20°C
  • Specific Heat Capacity
  • Thermal Conductivity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。