MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

Subscribe to FREE Trade Publications!

Hastelloy® C-4 alloy, 9.5 mm thick plate, heat treated at 1066°C, rapid quenched, tested at RT

 

Subcategory: Superalloy; Nickel Base

Key Words: ASME SB-622, ASME SB-626, UNS N06455, ASME SB-574, ASME SB-575, ASME SB-619, nickel alloy

Material Notes:
Nickel content to balance. High temperature stability even after aging in the 650-1040°C (1200-1900°F) range as evidenced by good ductility and corrosion resistance. Resists the formation of grain-boundary precipitates and is therefore suitable for use in most chemical process applications in the as-welded condition. C-4 resists stress-corrosion cracking and oxidizing atmospheres up to 1040°C (1900°F). It has exceptional resistance to hot contaminated mineral acids, solvents, chlorine and chlorine-contaminated media (organic and inorganic), dry chlorine, formic and acetic acids, acetic anhydride, seawater and brine solutions.

Data provided by the manufacturer, Haynes International, Inc.

Available Properties
  • Density
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • Modulus of Elasticity at Elevated Temperature
  • Electrical Resistivity
  • Electrical Resistivity at Elevated Temperature
  • CTE, linear 20°C
  • CTE, linear 250°C
  • CTE, linear 500°C
  • CTE, linear 1000°C
  • Specific Heat Capacity
  • Specific Heat Capacity at Elevated Temperature
  • Thermal Conductivity
  • Thermal Conductivity at Elevated Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。