Ametek PF35 Nickel Alloy Thermal Spray Powder

 

Subcategory: Superalloy; Nickel Base

Key Words: Powder metallurgy

Material Notes:
Nickel content above calculated as balance.

For coatings requiring intermediate hardness, excellent machinability and resistance to corrosion, heat and cracking. Use on shafts, sleeves, and wear surfaces.

Ametek has developed this and other engineering alloys for hardfacing - the process of spraying and fusing metal powder onto a workpiece or substrate to give it specific hardness, wear, or corrosion resistant properties. Ametek® powders are engineered to have the precise size, spherical shape, and low oxygen content required for optimal thermal spraying characteristics.

Information provided by Ametek Specialty Metal Products.

Available Properties
  • Hardness, Rockwell C
  • Melting Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。